Plak asye s460n

Aug 27, 2025 Kite yon mesaj

S460N - Z35 plak asye se yon asye Ewopeyen an estanda ak fòs segondè, espesyalman nan eta a nòmalize oswa nòmalize ak tanperaman, li gen pi wo pwopriyete konplè mekanik. S460N - Z35 Specification Pèfòmans: EN10025-3. Klas asye ki gen rapò yo se S460NL S420N S420NL S355N S355NL S275N S275NL.

 

Pwopriyete mekanik S460N - Z35 Steel Plate:
Sede fòs mwens pase oswa egal a 16mm: 460 MPa
Fòs sede 16-40mm: 440 MPa
Fòs sede 40-63mm: 430 MPa
Fòs sede 63-80mm: 410 MPa
Sede fòs 80-100mm: 400 MPa
Fòs sede 100-150mm: 380 MPa
Fòs rupture (MPa): 530-720 MPa
Elongasyon yon%: 17

 

Konpozisyon chimik nan S460N - Z35 Plak Steel:
C: mwens pase oswa egal a 0.20; SI: mwens pase oswa egal a 0.60; MN: 1.00-1.70; P: mwens pase oswa egal a 0.030; S: Mwens pase oswa egal a 0.025; NI: mwens pase oswa egal a 0.80; CR: mwens pase oswa egal a 0.30; MO: mwens pase oswa egal a 0.10; Cu: mwens pase oswa egal a 0.55; NB: mwens pase oswa egal a 0.05; V: mwens pase oswa egal a 0.20; Ti: mwens pase oswa egal a 0.05; AL: pi gran pase oswa egal a 0.02; N: mwens pase oswa egal a 0.025

S460N - Z35 plak asye se sitou itilize fè bato gwo, pon, ekipman estasyon pouvwa, mwayen ak chodyèr presyon segondè, veso presyon ki wo, stock woule, machin monte, machin min ak lòt gwo pati soude estriktirèl.

 

wechat2025-07-09174549751

 

S460n asye plak livrezon kondisyon entwodiksyon

Estanda EN10025 la espesifye ke plak asye S460N dwe delivre nan kondisyon normalized oswa normalized - woule anba pwosesis ekivalan.

Aplikasyon S460N:

Plak S460N asye ki dwe nan asye fasilman ak machinabl, prezante segondè fòs sede ak rezistans fatig. Pwopriyete li yo vin pi estab apre tretman chalè, fè li lajman itilize nan machin min, machin jeni, konstriksyon bato, estrikti pon, ak konstriksyon bilding.

S460N asye plak dimansyon estanda (epesè*lajè*longè / inite: mm)

8mm*2000mm*12000mm
8mm*2500mm*12000mm
10mm*2000mm-2500mm*12000mm
12mm*1800mm-2500mm*12000mm
14mm*1500mm-2850mm*12000mm
16mm*1450mm-3000mm*12000mm
18mm*1000mm-3000mm*11500mm
20mm*1450mm-3200mm*12000mm
22mm*1100mm-2500mm*12000mm
24mm*1000mm-3500mm*13500mm
26mm*1470mm-3500mm*13500mm
28mm*1000mm-3500mm*12500mm
30mm*1250mm-3000mm*12500mm
32mm*1410mm-3250mm*12000mm
35mm*1000mm-2500mm*12100mm
40mm*1210mm-3000mm*10000mm
45mm*1000mm-2500mm*12000mm
Pi gran pase oswa egal a 50mm*1000mm-3000mm*100mm-12500mm