Lwil oliv ak plat platfòm asye plak S420G 1+ M posede fòs la sede minimòm nan 420MPA, ak fòs la rupture yo dwe pi wo a 500 MPA.TMCP tretman chalè ki nesesè pou asye plak S420G 1+ M pou nenpòt ki epesè lè woule.

 

Steel Creole: EN 10225

Kalite woule: lwil oliv ak plat platfòm asye plak

Epesè: 6mm-300mm

Lajè: 1500mm-4200mm

Longè: 3000mm-18000mm

Tretman chalè: Thermo - Pwosesis kontwòl mekanik (TMCP)

 

Pwopriyete mechnical pou s420g 1+ m plak asye:

Epesè (mm)
S420G1+M Mwens pase oswa egal a 16 >16 mwens pase oswa egal a 40 >40 mwens pase oswa egal a 63 >63 mwens pase oswa egal a 80 > 80
Sede fòs (pi gran pase oswa egal a MPa) 420 400 390 380 380
  Mwens pase oswa egal a 40 > 40
Fòs rupture (MPa) 500 480


Konpozisyon chimik pou s420g 1+ m plak asye (analiz louch max%)
 

Main eleman chimik konpozisyon nan s420g 1+ m asye plak
C Si Mn P S Cr Mwa Nb+v Nb+v+ti
0.14 0.15-0.55 1.65 0.020 0.010 0.25 0.25 0.09 0.11
NI T CU N NB Ti V Cr+mo+ni+cu
0.70 0.015-0.055 0.30 0.010 0.040 0.025 0.080 0.90

 

S420g 1+ M platfòm plato asye lòt non lòt

S420G 1+ M Platfòm Platfòm Plak,

S420G 1+ M Offshore Plak Steel estrikti,

S420G 1+ M Platfòm Platfòm Plak,

S420G 1+ M Welding Plak Steel estriktirèl.

Lòt kondisyon

UT (egzamen ultrasons), AR (tankou cho woule sèlman), TMCP (tèmik pwosesis kontwòl mekanik), N (normalized), Q+T (pasè ak apeze), z tès direksyon (Z15, Z25, Z35), Charpy V - tès enpak, tankou SG.