EN10149-2 S315MC asye plak / fèy, EN10149-2 S315MCsteel plak / fèy, anba estanda EN, nou ka konsidere S315MC asye plak / fèy pou segondè sede fòs frèt fòme asye.
S315MC asye plakse yon kondisyon livrezon teknik pou segondè sede fòs frèt fòme asye.Se selon EN10149 -2 standard.we ka konsidere S315MC asye plak / fèy yo ba -pèlit asye klas ofri ekselan koube, flange, frèt-borderingand plisman pwopriyete nan tou de direksyon longitudinal ak transverse.
S315MC konpozisyon chimik ak pwopriyete mekanik
|
S315MC Konpozisyon chimik |
|||||
|
Klas |
Eleman Max (%) |
||||
|
S315MC
|
C |
Si |
Mn |
P |
S |
|
Mwens pase oswa egal a 0.12 |
Mwens pase oswa egal a 0.50 |
Mwens pase oswa egal a 1.30 |
Mwens pase oswa egal a 0.025 |
Mwens pase oswa egal a 0.020 |
|
|
Alt |
Nb |
V |
Ti |
|
|
|
Pi gran pase oswa egal a 0.015 |
Mwens pase oswa egal a 0.09 |
Mwens pase oswa egal a 0.20 |
0.15 |
|
|
|
Klas |
Tensile (Mpa) |
Sede (Min Mpa) |
Pwolonjman (min%) |
Epesè (mm) |
|
S315MC |
390-510 |
Pi gran pase oswa egal a 315 |
Pi gran pase oswa egal a 20 |
<3.0 |
|
Pi gran pase oswa egal a 24 |
Pi gran pase oswa egal a 3.0 |
Klas ekivalan nanS315MC asye plak
|
Inyon Ewopeyen |
USA |
Almay |
Japon |
Lafrans |
Angletè |
Espay |
|
S315MC |
1392 |
QstE300TM |
SPFH490 |
E315D |
43F30 |
AE275HC |
Karakteristik kle nan EN 10149-2 S315MC Plak
Segondè fòs rupture: plak sa yo bay ekselan fòs rupture, sa ki pèmèt konsepsyon an nan pwodwi pi lejè ak pi efikas ak estrikti.- Rezistans abrasion: alyaj yo itilize nan plak sa yo amelyore dite yo ak severite, fè yo rezistan a mete ak fwotman.
- Fòmabilite: Plak EN 10149-2 S315MC yo trè fòmab, sa ki pèmèt fasil fòme ak fabrikasyon nan divès eleman ak estrikti.
- Rezistans move tan: Plak sa yo montre bon rezistans move tan, ki fè yo apwopriye pou aplikasyon pou deyò ak anviwònman.
- Konpozisyon chimik: Fè soti nan kabòn, Silisyòm, Manganèz, fosfò, souf, aliminyòm, ak nikèl, plak sa yo ofri yon konpozisyon balanse pou redwi frajil ak amelyore pwopriyete mekanik.
- Rezistans korozyon: Plak sa yo fèt pou kenbe tèt ak estrès mekanik ak fluctuations tanperati, sa ki fè yo ideyal pou anviwònman korozivite.
Aplikasyon nan EN 10149-2 S315MC Plak
- Pati otomobil: Yo itilize pou fabrike wou machin, ankadreman, ak lòt konpozan akòz kontni segondè kabòn yo ak rezistans nan mete.
- Eleman estriktirèl: Ideyal pou eleman estriktirèl ki mande gwo -fòs ak ba-alyaj asye, tankou pon, bato, ak bilding.
- Faktori: Lajman itilize nan pwosesis fabrikasyon pou veso presyon, konpozan machin, ak ekipman endistriyèl.
- Konstriksyon: Apwopriye pou aplikasyon konstriksyon ki mande materyèl dirab ak move tan -rezistan.
- Amardeep Steel se yon manifakti dirijan nan plak EN 10149-2 S315MC, ki ofri bon jan kalite siperyè ak fyab pou pwojè ou yo. Plak sa yo disponib nan diferan gwosè, konpozisyon chimik, ak pwopriyete mekanik pou satisfè divès kondisyon endistriyèl. Mete konfyans nou nan ekspètiz nou an epi chwazi Plak EN 10149-2 S315MC pou pèfòmans eksepsyonèl ak rezistans nan aplikasyon ou yo.
Kondisyon adisyonèl
UT (Egzamen Ultrasonic), AR (Kòm woule cho sèlman), TMCP (Tèmik Pwosesis kontwòl mekanik), N (Normalize), Q + T (Tenn ak Tanperaman), Tès Direksyon Z (Z15, Z25, Z35), Tès Enpak Charpy V - Notch, Tès Twazyèm Pati (tankou Tès SGS), kouvwi ak pating.
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com.Nou plis ke kontan ede ou.


| Klas Kabòn ak Ba-alyaj segondè-Fòs Asye ki founi pa GNEE | |||||
| ASTM/ASME | ASTM A36/A36M | ASTM A36 | |||
| ASTM A283/A283M | ASTM A283 Klas A | ASTM A283 Klas B | ASTM A283 Klas C | ASTM A283 Klas D | |
| ASTM A514/A514M | ASTM A514 Klas A | ASTM A514 Klas B | ASTM A514 Klas C | ASTM A514 Klas E | |
| ASTM A514 Klas F | ASTM A514 Klas H | ASTM A514 klas J | ASTM A514 Klas K | ||
| ASTM A514 Klas M | ASTM A514 Klas P | ASTM A514 Klas Q | ASTM A514 Klas R | ||
| ASTM A514 Klas S | ASTM A514 Klas T | ||||
| ASTM A572/A572M | ASTM A572 Klas 42 | ASTM A572 Klas 50 | ASTM A572 Klas 55 | ASTM A572 Klas 60 | |
| ASTM A572 Klas 65 | |||||
| ASTM A573/A573M | ASTM A573 Klas 58 | ASTM A573 Klas 65 | ASTM A573 Klas 70 | ||
| ASTM A588/A588M | ASTM A588 Klas A | ASTM A588 Klas B | ASTM A588 Klas C | ASTM A588 Klas K | |
| ASTM A633/A633M | ASTM A633 Klas A | ASTM A633 Klas C | ASTM A633 Klas D | ASTM A633 Klas E | |
| ASTM A656/A656M | ASTM A656 Klas 50 | ASTM A656 Klas 60 | ASTM A656 Klas 70 | ASTM A656 Klas 80 | |
| ASTM A709/A709M | ASTM A709 Klas 36 | ASTM A709 Klas 50 | ASTM A709 Klas 50S | ASTM A709 Klas 50W | |
| ASTM A709 klas HPS 50W | ASTM A709 klas HPS 70W | ASTM A709 Klas 100 | ASTM A709 Klas 100W | ||
| ASTM A709 klas HPS 100W | |||||
| ASME SA36/SA36M | ASME SA36 | ||||
| ASME SA283/SA283M | ASME SA283 Klas A | ASME SA283 Klas B | ASME SA283 Klas C | ASME SA283 Klas D | |
| ASME SA514/SA514M | ASME SA514 Klas A | ASME SA514 Klas B | ASME SA514 Klas C | ASME SA514 Klas E | |
| ASME SA514 Klas F | ASME SA514 Klas H | ASME SA514 Klas J | ASME SA514 Klas K | ||
| ASME SA514 Klas M | ASME SA514 Klas P | ASME SA514 Klas Q | ASME SA514 Klas R | ||
| ASME SA514 Klas S | ASME SA514 Klas T | ||||
| ASME SA572/SA572M | ASME SA572 Klas 42 | ASME SA572 Klas 50 | ASME SA572 Klas 55 | ASME SA572 Klas 60 | |
| ASME SA572 Klas 65 | |||||
| ASME SA573/SA573M | ASME SA573 Klas 58 | ASME SA573 Klas 65 | ASME SA573 Klas 70 | ||
| ASME SA588/SA588M | ASME SA588 Klas A | ASME SA588 Klas B | ASME SA588 Klas C | ASME SA588 Klas K | |
| ASME SA633/SA633M | ASME SA633 Klas A | ASME SA633 Klas C | ASME SA633 Klas D | ASME SA633 Klas E | |
| ASME SA656/SA656M | ASME SA656 Klas 50 | ASME SA656 Klas 60 | ASME SA656 Klas 70 | ASME SA656 Klas 80 | |
| ASME SA709/SA709M | ASME SA709 Klas 36 | ASME SA709 Klas 50 | ASME SA709 Klas 50S | ASME SA709 Klas 50W | |
| ASME SA709 klas HPS 50W | ASME SA709 klas HPS 70W | ASME SA709 Klas 100 | ASME SA709 Klas 100W | ||
| ASME SA709 klas HPS 100W | |||||
| EN10025 | EN10025-2 | EN10025-2 S235J0 | EN10025-2 S275J0 | EN10025-2 S355J0 | EN10025-2 S355K2 |
| EN10025-2 S235JR | EN10025-2 S275JR | EN10025-2 S355JR | EN10025-2 S420J0 | ||
| EN10025-2 S235J2 | EN10025-2 S275J2 | EN10025-2 S355J2 | |||
| EN10025-3 | EN10025-3 S275N | EN10025-3 S355N | EN10025-3 S420N | EN10025-3 S460N | |
| EN10025-3 S275NL | EN10025-3 S355NL | EN10025-3 S420NL | EN10025-3 S460NL | ||
| EN10025-4 | EN10025-4 S275M | EN10025-4 S355M | EN10025-4 S420M | EN10025-4 S460M | |
| EN10025-4 S275ML | EN10025-4 S355ML | EN10025-4 S420ML | EN10025-4 S460ML | ||
| EN10025-6 | EN10025-6 S460Q | EN10025-6 S460QL | EN10025-6 S460QL1 | EN10025-6 S500Q | |
| EN10025-6 S500QL | EN10025-6 S500QL1 | EN10025-6 S550Q | EN10025-6 S550QL | ||
| EN10025-6 S550QL1 | EN10025-6 S620Q | EN10025-6 S620QL | EN10025-6 S620QL1 | ||
| EN10025-6 S690Q | EN10025-6 S690QL | EN10025-6 S690Q1 | EN10025-6 S890Q | ||
| EN10025-6 S890QL | EN10025-6 S890QL1 | EN10025-6 S960Q | EN10025-6 S960QL | ||
| JIS | JIS G3101 | JIS G3101 SS330 | JIS G3101 SS400 | JIS G3101 SS490 | JIS G3101 SS540 |
| JIS G3106 | JIS G3106 SM400A | JIS G3106 SM400B | JIS G3106 SM400C | JIS G3106 SM490A | |
| JIS G3106 SM490YA | JIS G3106 SM490B | JIS G3106 SM490YB | JIS G3106 SM490C | ||
| JIS G3106 SM520B | JIS G3106 SM520C | JIS G3106 SM570 | |||
| DIN | DIN 17100 | DIN17100 St52-3 | DIN17100 St37-2 | DIN17100 St37-3 | DIN17100 RSt37-2 |
| DIN17100 USt37-2 | |||||
| DIN 17102 | DIN17102 StE315 | DIN17102 EStE315 | DIN17102 TStE315 | DIN17102 WStE315 | |
| DIN17102 StE355 | DIN17102 EStE355 | DIN17102 TStE355 | DIN17102 WStE355 | ||
| DIN17102 StE380 | DIN17102 EStE380 | DIN17102 TStE380 | DIN17102 WStE380 | ||
| DIN17102 StE420 | DIN17102 EStE420 | DIN17102 TStE420 | DIN17102 WStE420 | ||
| DIN17102 StE460 | DIN17102 EStE460 | DIN17102 TStE460 | DIN17102 WStE460 | ||
| DIN17102 StE500 | DIN17102 EStE500 | DIN17102 TStE500 | DIN17102 WStE500 | ||
| DIN17102 EStE285 | |||||
| GB | GB/T700 | GB/T700 Q235A | GB/T700 Q235B | GB/T700 Q235C | GB/T700 Q235D |
| GB/T700 Q275 | |||||
| GB/T1591 | GB/T1591 Q345A | GB/T1591 Q390A | GB/T1591 Q420A | GB/T1591 Q420E | |
| GB/T1591 Q345B | GB/T1591 Q390B | GB/T1591 Q420B | GB/T1591 Q460C | ||
| GB/T1591 Q345C | GB/T1591 Q390C | GB/T1591 Q420C | GB/T1591 Q460D | ||
| GB/T1591 Q345D | GB/T1591 Q390D | GB/T1591 Q420D | GB/T1591 Q460E | ||
| GB/T1591 Q345E | GB/T1591 Q390E | ||||
| GB/T16270 | GB/T16270 Q550C | GB/T16270 Q550D | GB/T16270 Q550E | GB/T16270 Q550F | |
| GB/T16270 Q620C | GB/T16270 Q620D | GB/T16270 Q620E | GB/T16270 Q620F | ||
| GB/T16270 Q690C | GB/T16270 Q690D | GB/T16270 Q690E | GB/T16270 Q690F | ||
| GB/T16270 Q800C | GB/T16270 Q800D | GB/T16270 Q800E | GB/T16270 Q800F | ||
| GB/T16270 Q890C | GB/T16270 Q890D | GB/T16270 Q890E | GB/T16270 Q890F | ||
| GB/T16270 Q960C | GB/T16270 Q960D | GB/T16270 Q960E | GB/T16270 Q960F | ||
| GB/T16270 Q500 | |||||