S275ML ​​asye plak

Oct 13, 2025 Kite yon mesaj

Steel Creole: EN 10025-4

Kalite woule: plak asye estriktirèl, plak asye alyaj ki ba

Epesè: 6mm-500mm

Lajè: 1500mm-4200mm

Longè: 3000mm-18000mm

Tretman chalè: Thermo-Prosesis kontwòl mekanik (TMCP)

 

Se estriktirèl S275ML, S275ML STEEL PLATE, S275ML STEEL SHEET sitou itilize pou ankadreman asye, konstriksyon asye, ray tren ak pati machin ki ta dwe nan tanperati ki ba. 20 santigree.When woule plak asye S275ML, kontni P ak S yo ka 0.005% pi wo pase valè tablo ki anba yo.

 

Pwopriyete mekanik pou plak asye S275ML:
 

Epesè (mm)
S275ML Mwens pase oswa egal a 16 >16 Mwens oswa egal a 40 >40 Mwens pase oswa egal a 63 >63 Mwens pase oswa egal a 80 >80 Mwens pase oswa egal a 100 > 100
Fòs sede (pi gran pase oswa egal a Mpa) 275 265 255 245 245 240
  Mwens pase oswa egal a 40 >40 Mwens pase oswa egal a 63 >63 Mwens pase oswa egal a 80 >80 Mwens pase oswa egal a 100 > 100
Fòs rupture (Mpa) 370-530 360-520 350-510 350-510 350-510


 

Konpozisyon chimik pou plak asye S275ML ​​(Analiz Chalè Max%)

 

 

Pwensipal eleman chimik konpozisyon plak asye S275ML
C Si Mn P S Nb V
0.13 0.50 1.50 0.025 0.020 0.05 0.08
Al(total) Ti Kr Ni Mo Cu N
Pi gran pase oswa egal a 0.02 0.05 0.30 0.30 0.10 0.55 0.015