Konpozisyon chimik (EN 10025-2)
| Eleman | Pousantaj (%) |
|---|---|
| Kabòn (C) | Mwens pase oswa egal a 0.22 |
| Manganèz (MN) | Mwens pase oswa egal a 1.50 |
| Fosfò (P) | Mwens pase oswa egal a 0.035 |
| Souf (yo) | Mwens pase oswa egal a 0.035 |
| Silisyòm (SI) | Mwens pase oswa egal a 0.55 |
Pwopriyete mekanik
| Posesyon | Valè |
|---|---|
| Sede fòs | 275 MPa (min) |
| Fòs rupture | 410-560 MPa |
| Elongasyon | 20-23% (nan 50mm) |
| Enpak enèji | 27 J nan +20 degre |
| Sede fòs (pi gran pase oswa egal a N/mm2) | Fòs rupture | |||||||
| Kanpay | Klas asye | d mwens pase oswa egal a 16 | 16 | 40 | 60 | 100 | 150 | N/mm2 |
|
| Pòslèn | Q235 | 235 | 225 | 215 | 215 | 195 | 185 | 370-500 |
| Nou | A36 | 250 MPa (D mwens pase oswa egal a 200mm) | 400-550 | |||||
| Eropeyèn | S235 | 235 | 225 | 215 | 215 | 195 | 185 | 360-510 |
| Japon | SS400 | 245 | 235 | 215 | 215 | 205 | 205 | 400-510 |

Plak asye S275JR, akòz modere li yo segondè fòs, andirans, rezistans fatig, rezistans enpak, rezistans korozyon, weldability, ak fasilite nan pwosesis - Comprehensive segondè - Pwopriyete bon jan kalite - te toujou resevwa lwanj ki gaye toupatou ak nan men fabrikasyon an pou an. Imedyatman, akòz rekonesans sosyete a ak anpil itilizasyon li yo nan manifakti, makonnen ak optimize kontinyèl ak amelyore nan materyèl la pa pwodiktè, S275JR plak asye te piti piti vin youn nan klas yo asye souvan itilize nan Lachin.