Q420A Adopte estanda: GB-T1591 Espesifikasyon Creole se pou asye woule pou estrikti soude
Q420A spesifikasyon:
Epesè: 1mm a 500mm
Lajè: 1500mm a 4500mm
Longè: 3000mm a 27000mm
Enspeksyon Twazyèm Pati pou Q420A: ABS, DNV, BV, GL, CCS, LR, RINA, KR, NK, CE, SGS, IKE, IEI oswa lòt depatman kalite.
Q420A konpozisyon chimikMax % nan analiz pwodwi klas la
|
C |
Si |
Mn |
P |
S |
Nb |
V |
Ti |
|
0.20 |
0.50 |
1.70 |
0.035 |
0.035 |
0.07 |
0.20 |
0.20 |
|
Kr |
Ni |
Cu |
N |
Mo |
B |
Epitou min |
|
|
0.30 |
0.80 |
0.30 |
0.015 |
0.20 |
- |
- |
|
Q420A Sede fòs
|
Epesè nominal (mm) |
Pou 16 |
16-40 |
40-63 |
63-80 |
80- 100 |
100- 150 |
150- 200 |
200- 250 |
250- 400 |
|
ReH - Minimòm fòs sede (MPa) |
420 |
400 |
380 |
360 |
360 |
340 |
- |
- |
- |
Q420A Fòs Tensile
|
Epesè nominal (mm) |
Pou 40 |
40-63 |
63-80 |
80-100 |
100-150 |
150-250 |
250-400 |
|
ReH - Minimòm fòs sede (MPa) |
520-680 |
520-680 |
520-680 |
520-680 |
500-650 |
- |
- |
Q420A Enpak Tès degre ak enèji
|
|
Min Enèji Nominal epesè |
||
|
Degre tanperati |
- |
||
|
Epesè (mm) |
12-150 |
150-250 |
250-400 |
|
Tès enpak Notch. Min. enèji absòbe |
- |
- |
- |
Aplikasyon
Plak asye Q420A yo itilize nan konstriksyon pon, konstriksyon otowout ak lòt konstriksyon Jeni