Q345 seri asye gen ladan Q345A, Q345B, Q345C, Q345D, ak Q345E, kote Q reprezante fòs sede a, nimewo 345 lèt la reprezante valè pwen sede (nan MPa), ak lèt ​​yo A, B, C, D, ak E respektivman reprezante tanperati ki ba - nan enpak la diferan tanperati enpak, rezistans prensipal la nan asye a. Nan ti bout tan, Q345A pa fè enpak; Q345B, enpak tanperati chanm 20 degre; Q345C, enpak 0 degre; Q345D, -20 degre enpak; Q345E, -40 enpak. Diferan tanperati enpak, valè enpak tou diferan.

 

Pwopriyete kle

Fòs Sede: Min 345 MPa (pou epesè mwens pase oswa egal a 16mm).

Fòs rupture: 470-630 MPa.

Klas: A, B, C, D, E (divès tès enpak).

Karakteristik: ekselan soudabilite, bon fòmabilite, severite.

Klas yo eksplike (A rive E)

Q345A: Klas debaz, pa gen okenn tès enpak espesifik.

Q345B: Tès enpak nan 0 degre (34 J).

Q345C: Tès enpak nan 0 degre (34 J).

Q345D: Tès enpak nan -20 degre (34 J).

Q345E: Tès enpak nan -40 degre (27 J).

 

Aplikasyon komen

Estrikti bilding yo

Konstriksyon pon

Machin lou

Pwojè Jeni

 

KONPOZISYON CHIMIK Q345 SERIES STEEL

 

Materyèl

C

Si

Mn

P

S

Ni

Kr

Cu:

V

Q345A

0.12-0.2

0.20-0.6

1.00-1.6

Mwens pase oswa egal a 0.045

Mwens pase oswa egal a 0.045

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.2

0.02-0.15

Q345B

0.12-0.2

0.20-0.6

1.00-1.6

Mwens pase oswa egal a 0.04

Mwens pase oswa egal a 0.04

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.2

0.02-0.15

Q345C

0.12-0.2

0.20-0.6

1.00-1.6

Mwens pase oswa egal a 0.035

Mwens pase oswa egal a 0.035

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.2

0.02-0.15

Q345D

Mwens pase oswa egal a 0.18

0.20-0.6

1.00-1.6

Mwens pase oswa egal a 0.03

Mwens pase oswa egal a 0.03

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.2

0.02-0.15

Q345E

Mwens pase oswa egal a 0.18

0.20-0.6

1.00-1.6

Mwens pase oswa egal a 0.025

Mwens pase oswa egal a 0.025

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.3

Mwens pase oswa egal a 0.2

0.02-0.15

 

PWOPRIYETE MECHANIK Q345 SERIES STEEL

 

Materyèl

Fòs rupture, Mpa

Sede fòs, Mpa

Elongasyon

Q345A

490-675

Pi gran pase oswa egal a 345

Pi gran pase oswa egal a 21

Q345B

490-675

Pi gran pase oswa egal a 345

Pi gran pase oswa egal a 21

Q345C

490-675

Pi gran pase oswa egal a 345

Pi gran pase oswa egal a 22

Q345D

490-675

Pi gran pase oswa egal a 345

Pi gran pase oswa egal a 22

Q345E

490-675

Pi gran pase oswa egal a 345

Pi gran pase oswa egal a 22