P460NH se yon plak asye estanda Ewopeyen an pou veso presyon. "460" endike fòs sede li yo nan MPa, ak "N" vle di ke se plak la asye lage nan kondisyon normalized oswa nòmalize woule.

 

Kondisyon chimik yo
(analiz jete, % pa mas, maksimòm pèmèt sof si endike otreman)

C Si Mn P S Al total N Cr CU Mwa NB NI Ti V Nb+ti+v
0.20 0.60 1.10 – 1.70 0.025 0.015 0.020 min 0.025 0.30 0.70 0.10 0.05 0.80 0.03 0.20 0.22

Kondisyon rupture

Epesè pwodwi Sede fòs MPA Rupture fòs MPA Elongasyon yon%
jiska 16mm 460 min 570 – 730 17 min
16mm a 40mm 445 min 570 – 720 17 min
Plis pase 40mm a 60mm 430 min 570 a 720 17 min
Plis pase 60mm a 100mm 400 min 540 a 710 17 min

Enpak valè enèji pou kondisyon an normalized

  -20 degre 0 degre +20 degre
Transverse 30 J min 40 J min 50 J min
Lonitudinal 45 J min 65 J min 75 J min

Min. Valè pou prèv fòs RP0,2 (MPa) nan tanperati ki wo

Epesè 50 degre 100 degre 150 degre 200 degre 250 degre 300 degre 350 degre 400 degre
jiska 16mm 445 419 388 356 326 300 278 261
16mm a 40mm 430 405 375 345 316 290 269 253
Plis pase 40mm a 60mm 416 391 362 333 305 281 260 244
Plis pase 60mm a 100mm 387 364 337 310 284 261 242 227

 

wechat2025-07-11112506516

Souvan ranpli dimansyon ak espesifikasyon

P460NH 10*2000-2400*9000-12000

P460NH 12*2200-2500*10000-13500

P460NH 15*2000-2500*9000-11500

P460NH 18*1800-2800*9000-12500

P460NH 20*2000-2400*9000-12000

P460NH 22*2300-2500*10000-13000

P460NH 25*2000-2500*9000-11500

P460NH 30*2000-2400*9000-12000

P460NH 35*1840-2600*9000-11500

P460NH 40*2000-2700*9500-12000

P460NH 50*2000-2700*9000-11500

P460NH 60*1850-2800*8700-12000