P420ML1 ak P420ML2yo tou de plak asye thermomechanically woule pou veso presyon ak chodyèr, dapre EN 10028 -5 estanda. Diferans kle a se rezistans enpak ba-tanperati yo: P420ML1 espesifye pou tès enpak nan-40 degre, pandan y ap P420ML2 espesifye pou tès enpak nan-50 degre. Tou de klas yo gen yon fòs sede minimòm de 420 MPa ak bon soudabilite.
EN10028-5 spesifikasyon estanda pou asye grenn amann soude, thermomechanically woule.
EN10028-5 kouvri klas asye yo bay nan twa kalite:
a) seri debaz yo (P...M)
b) seri ak pwopriyete tanperati ki ba jiska -40 degre (P ... ML1);
c) seri ak pwopriyete tanperati ki ba jiska -50 degre (P...ML2).
Teknoloji Siplemantè: Tès HIC|NACE MR0175|Z15|Z25|Z35
Epesè: 6MM a 300MM,
Lajè: 1500mm a 4050mm,
Longè: 3000mm a 15000mm
Pwopriyete mekanik pou plak asye P420ML1
| Epesè (mm) | Fòs sede (pi gran pase oswa egal a Mpa) | Fòs rupture (Mpa) | Elongasyon nan pi gran pase oswa egal a,% |
| T Mwens pase oswa egal a 16 | 420 | 500-660 | 19 |
| 16<> | 400 | ||
| 40<> | 390 |
Konpozisyon chimik pou plak asye P420ML1 (Analiz Chalè Max%)
| Pwensipal eleman chimik konpozisyon plak asye P420ML1 | ||||||
| C | Si | Mn | P | S | Al (total) | N |
| 0.16 | 0.50 | 1.70 | 0.020 | 0.015 | Pi gran pase oswa egal a 0.020 | 0.020 |
| Mo | Nb | Ni | Ti | V | Cr+Cu+Mo | |
| 0.20 | 0.05 | 0.50 | 0.05 | 0.10 | 0.60 | |
Pwopriyete mekanik pou plak asye P420ML2:
| Epesè (mm) | Fòs sede (pi gran pase oswa egal a Mpa) | Fòs rupture (Mpa) | Elongasyon nan pi gran pase oswa egal a,% |
| T Mwens pase oswa egal a 16 | 420 | 500-660 | 19 |
| 16<> | 400 | ||
| 40<> | 390 |
Konpozisyon chimik pou plak asye P420ML2 (Analiz Chalè Max%)
| Pwensipal eleman chimik konpozisyon plak asye P420ML2 | ||||||
| C | Si | Mn | P | S | Al (total) | N |
| 0.16 | 0.50 | 1.70 | 0.020 | 0.015 | Pi gran pase oswa egal a 0.020 | 0.020 |
| Mo | Nb | Ni | Ti | V | Cr+Cu+Mo | |
| 0.20 | 0.05 | 0.50 | 0.05 | 0.10 | 0.60 | |
Kondisyon teknik ak sèvis adisyonèl pou plak asye P420ML1/ML2
♦ Tès tansyon wo
♦ Ba tanperati enpak tès
♦ Tretman chalè simule -soude (PWHT)
♦ Tès ultrasons anba EN 10160, ASTM A435, A577, A578
♦ Li te bay sètifika tès orijinal Mill anba EN 10204 FÒMA 3.1/3.2
♦ Piki eksplozif ak Penti, Koupe ak soude dapre demann itilizatè final la
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.
| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Klas3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||