Ki jan asye wo-fòs tankou CCS EH36/FH40 pwodwi nan Lachin fè an tèm de weldability ak pri compétitivité?

Aug 08, 2025 Kite yon mesaj

1. pèfòmans soude: ekivalan kabòn (CEV) ak kondisyon chofe

Chinwa CCS EH36/FH40 tipikman gen pi wo CEV, ogmante konpleksite soude.

Konparezon CEV:

Baowu eh36: CEV ~ 0.38-0.42(akòz pi wo C/MN kontni).

Posco EH36: CEV ~ 0.34-0.38(Chimi mèg ak microalloying).

Chofe enpak:

Chinwa EH36 souvan mande pou100-125 degre chofe(vs . 75 - 100 degre pou EH36 Koreyen).

Ka etid: Cosco rapò10–15% pi long fwa soudepou Baowu EH36 vs POSCO.

Krak sansiblite:

Pi woPCM (Cracking Index)Nan asye Chinwa (0.22-0.25 vs . 0.18 - 0.21 pou JFE).

Rezilta: PlisIdwojèn-pwovoke fann (HIC) risk, mande kontwòl elektwòd sevè.


2. Pri competitiveness: avantaj pri ak komès-konpwomi

Chinwa CCS asye yo se 15-25% pi bon mache men fè fas a baryè ekspòtasyon.

Pri konparezon (FOB, 2024):

Baowu CCS EH36: $ 600-650/tòn.

POSCO ABS EH36: $ 750-800/tòn.

JFE DNV EH36: $ 800-850/tòn.

Chofè Pri:

BeseNi/cr alyajNan asye Chinwa diminye depans materyèl.

Sibvansyon Chinwa domestik(egzanp, repo taks pou eta-posede moulen).

Baryè komès:

Inyon Ewopeyen anti-moun ap jete fatra devwa (25%)Negate avantaj pri nan Ewòp.

Doub Sètifikasyon (CCS+ABS)ajoute$ 50-100/tònpou ekspòtasyon.

Mache reyalite: Bri ak domestik bato Chinwapriyorite Baowu/Ansteel; Flòt Global pito POSCO/JFE.


3. Weld consommables ak efikasite fabwikasyon

Asye Chinwa mande elektwòd espesyalize, ogmante depans fabwikasyon.

Konpatibilite konsomasyon:

Baowu EH36 souvan mande pouAWS E81T1-NI2(vs estanda E71T-1 pou POSCO).

Pri: Fil Ni ki baze sou yo20-30% pricier.

Otomatik soude konvnab:

Koreyen EH36pèfòme pi byen nanrobotized fcawAkòz pi ba spatter.

Moulen Chinwa yo ap amelyoreKonsistans TMCPPou diminye domaj soude.

SHIPYARD Feedback:

Samsung Heavy Industries rapò5-8% pi wo pousantaj echèk NDTak CCS FH40 vs POSCO.

Solisyon: Gen kèk yad Chinwa pre-tès plak akmetal filler matche.


4. Sètifikasyon Entènasyonal ak Pèsepsyon Kalite

ABS/DNV apwobasyon pou Chinwa EH36/FH40 lag dèyè asye Japonè/Koreyen.

Sètifikasyon obstakl:

Baowu aABS EH36egzijeTès enpak siplemantè(-40 degre Transverse).

DNV GL raman sètifye Ansteel FH40 pou transpòtè LNGsan done siplemantè.

Bon jan kalite repitasyon:

Posco a"Zewo Defèk" EH36se pi pito pou zòn kritik (egzanp, kale coamings).

Moulen Chinwa amelyore, men dout toujou nan mache Inyon Ewopeyen/US.

Egzanp Ka:

Newbuild Maersk a itilizeDoub-souse EH36(Posco Hull + Baowu klwazon).

Laas: Baowu envesti nanAI ki baze sou kontwòl kaliteKoresponn ak fyab JFE a.


5. Future Outlook: Amelyorasyon ak Green Steel Ras

Moulen Chinwa yo ap fèmen diferans lan via R&D ak inisyativ dirab.

Pwogrè TMCP:

Baowu aNouvo pakèt EH36reyalizeCEV 0.36(Pi pre Posco a 0.34).

Sib:Diminye chofe a 80 degrepa 2025.

Vèt asye pouse:

Baowu aIdwojèn ki baze sou DRI EH36(1.8t co₂/tòn) konkou ak Posco aHyundai wout EAF.

CCS plan notasyon asye ki ba-kabònaliman ak EU ETS.

Estrateji ekspòtasyon:

Doub-sètifye (CCS+ABS) EH36Pou Sidès Azyatik konstriksyon bato.

Pri undercuttingNan Lafrik/Amerik Latin nan.