EN10028-6 P460Q P460QH P460QL1 P460QL2 Euro-Estanda Plak asye wo-fòs

Oct 21, 2025 Kite yon mesaj

EN10028-6 P460Q presyon veso ak chodyè asye plak

 

EN10028-6 P460Qse yon estanda Ewopeyen an, ki gen gwo -fòs, ki ka soude amann-plak asye grenn ki te trempe ak tanperaman. Li konnen pou pwopriyete mekanik eksepsyonèl li yo epi yo itilize souvan nan konstriksyon ekipman tanperati ki wo ak veso presyon pou aplikasyon tankou lwil oliv, gaz, chodyèr, ak tank depo.

 

P460Q konpozisyon chimik

Klas

Eleman Max (%)

C

Si

Mn

P

S

N

B

P460Q

0.18

0.50

1.70

0.025

0.015

0.015

0.005

Mo

Cu

Nb

Ni

Ti

V

Zr

0.50

0.3

0.05

0.5

0.03

0.06

0.05

 

Klas

 

P460Q Pwopriyete mekanik

Epesè

Sede

Tensile

Elongasyon

P460Q

mm

Min Mpa

Mpa

% min

6-50

460

550-720

19%

50-100

440

550-720

19%

100-150

400

500-670

19%

 

Mande Yon Quote

 

EN10028-6 P460QH Presyon Veso ak Chodyè Steel Plak

 

EN10028-6 P460QHse yon asye ki trempe ak tanperaman, ki ka soude byen -pou presyon, li te ye pou fòs segondè li yo ak rezistans, patikilyèman nan tanperati ki ba. "P460" a endike yon fòs sede minimòm de 460MPa, ak "QH" espesifye yon -bon jan kalite rezistans tanperati ki ba teste nan−20∘𝐶. Yo itilize klas sa a pou aplikasyon tankou ekipman tanperati ki wo ak veso presyon.

 

P460QH konpozisyon chimik

Klas

Eleman Max (%)

C

Si

Mn

P

S

N

B

P460QH

0.18

0.50

1.70

0.025

0.015

0.015

0.005

Mo

Cu

Nb

Ni

Ti

V

Zr

0.50

0.3

0.05

0.5

0.03

0.06

0.05

 

Klas

 

P460QH Pwopriyete mekanik

Epesè

Sede

Tensile

Elongasyon

P460QH

mm

Min Mpa

Mpa

% min

6-50

460

550-720

19%

50-100

440

550-720

19%

100-150

400

500-670

19%

 

Mande Yon Quote

 

 

EN10028-6 P460QL1 Presyon Veso ak Chodyè Steel Plak

 

P460QL1se klas ki pi komen nan spesifikasyon EN10028_6, ki se yon kalite plak asye trempe ak trempe sitou gen entansyon pou bati chodyèr soude ak veso presyon.

 

P460QL1 konpozisyon chimik

Klas

Eleman Max (%)

C

Si

Mn

P

S

N

B

P460QL1

0.18

0.50

1.70

0.020

0.010

0.015

0.005

Mo

Cu

Nb

Ni

Ti

V

Zr

0.50

0.3

0.05

0.5

0.03

0.06

0.05

 

Klas

 

P460QL1 Pwopriyete mekanik

Epesè

Sede

Tensile

Elongasyon

P460QL1

mm

Min Mpa

Mpa

% min

6-50

460

550-720

19%

50-100

440

550-720

19%

100-150

400

500-670

19%

 

Mande Yon Quote

 

EN10028-6 P460QL2 Presyon Veso ak Chodyè Steel Plak

 

EN10028-6 P460QL2se yon klas asye ki ka soude, ki gen bon -granulman, ki trempe ak apeze pou itilize nan veso presyon ak ekipman tanperati ki wo-. "P460 la" refere a yon fòs sede minimòm de 460 MPa. Sifiks "QL2" la vle di ke asye a nòmal epi li gen yon enèji enpak minimòm -20degre.

 

P460QL2 konpozisyon chimik

Klas

Eleman Max (%)

C

Si

Mn

P

S

N

B

P460QL2

0.18

0.50

1.70

0.020

0.010

0.015

0.005

Mo

Cu

Nb

Ni

Ti

V

Zr

0.50

0.3

0.05

0.5

0.03

0.06

0.05

 

Klas

 

P460QL2 Pwopriyete mekanik

Epesè

Sede

Tensile

Elongasyon

P460QL2

mm

Min Mpa

Mpa

% min

6-50

460

550-720

19%

50-100

440

550-720

19%

100-150

400

500-670

19%

 

Mande Yon Quote

 

Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.

 

EN10028-6 P460QL2 Pressure Vessel And Boiler Steel Plate

EN10028-6 P460QL2 Pressure Vessel And Boiler Steel Plate

EN10028-6 P460QL2 Pressure Vessel And Boiler Steel Plate

 

Klas Plak Veso Presyon Apwovizyone Pa GNEE
ASTM ASTM A202/A202M ASTM A202 Klas A ASTM A202 Klas B    
ASTM A203/A203M ASTM A203 Klas A ASTM A203 Klas B ASTM A203 Klas D ASTM A203 Klas E
ASTM A203 Klas F      
ASTM A204/A204M ASTM A204 Klas A ASTM A204 Klas B ASTM A204 Klas C  
ASTM A285/A285M ASTM A285 Klas A ASTM A285 Klas B ASTM A285 Klas C  
ASTM A299/A299M ASTM A299 Klas A ASTM A299 Klas B    
ASTM A302/A302M ASTM A302 Klas A ASTM A302 Klas B ASTM A302 Klas C ASTM A302 Klas D
ASTM A387/A387M ASTM A387 Klas 5 Klas1 ASTM A387 Klas 5 Klas2 ASTM A387 Klas 11 Klas1 ASTM A387 Klas 11 Klas2
ASTM A387 Klas 12 Klas1 ASTM A387 Klas 12 Klas2 ASTM A387 Klas 22 Klas1 ASTM A387 Klas 22 Klas2
ASTM A515/A515M ASTM A515 Klas 60 ASTM A515 Klas 65 ASTM A515 Klas 70  
ASTM A516/A516M ASTM A516 Klas 55 ASTM A516 Klas 60 ASTM A516 Klas 65 ASTM A516 Klas 70
ASTM A517/A517M ASTM A517 Klas A ASTM A517 Klas B ASTM A517 Klas E ASTM A517 Klas F
ASTM A517 Klas P ASTM A517 klas J    
ASTM A533/A533M ASTM A533 Klas A Klas 1 ASTM A533 Klas B Klas1 ASTM A533 Klas C Class1 ASTM A533 Klas D Class1
ASTM A533 Klas A Klas2 ASTM A533 Klas B Klas2 ASTM A533 Klas C Class2 ASTM A533 Klas D Klas2
ASTM A533 Klas A Klas3 ASTM A533 Klas B Klas3 ASTM A533 Klas C Klas3 ASTM A533 Klas D Class3
ASTM A537/A537M ASTM A537 Klas 1 ASTM A537 Klas 2 ASTM A537 Klas 3  
ASTM A612/A612M ASTM A612      
ASTM A662/A662M ASTM A662 Klas A ASTM A662 Klas B ASTM A662 Klas C  
EN EN10028-2 EN10028-2 P235GH EN10028-2 P265GH EN10028-2 P295GH EN10028-2 P355GH
EN10028-2 16MO3      
EN10028-3 EN10028-3 P275N EN10028-3 P275NH EN10028-3 P275NL1 EN10028-3 P275NL2
EN10028-3 P355N EN10028-3 P355NH EN10028-3 P355NL1 EN10028-3 P355NL2
EN10028-3 P460N EN10028-3 P460NH EN10028-3 P460NL1 EN10028-3 P460NL2
EN10028-5 EN10028-5 P355M EN10028-5 P355ML1 EN10028-5 P355ML2 EN10028-5 P420M
EN10028-5 P420ML1 EN10028-5 P420ML2 EN10028-5 P460M EN10028-5 P460ML1
EN10028-5 P460ML2      
EN10028-6 EN10028-6 P355Q EN10028-6 P460Q EN10028-6 P500Q EN10028-6 P690Q
EN10028-6 P355QH EN10028-6 P460QH EN10028-6 P500QH EN10028-6 P690QH
EN10028-6 P355QL1 EN10028-6 P460QL1 EN10028-6 P500QL1 EN10028-6 P690QL1
EN10028-6 P355QL2 EN10028-6 P460QL2 EN10028-6 P500QL2 EN10028-6 P690QL2
JIS JIS G3115 JIS G3115 SPV235 JIS G3115 SPV315 JIS G3115 SPV355 JIS G3115 SPV410
JIS G3115 SPV450 JIS G3115 SPV490    
JIS G3103 JIS G3103 SB410 JIS G3103 SB450 JIS G3103 SB480 JIS G3103 SB450M
JIS G3103 SB480M      
GB GB713 GB713 Q245R GB713 Q345R GB713 Q370R GB713 12Cr1MoVR
GB713 12Cr2Mo1R GB713 13MnNiMoR GB713 14Cr1MoR GB713 15CrMoR
GB713 18MnMoNbR      
GB3531 GB3531 09MnNiDR GB3531 15MnNiDR GB3531 16MnDR  
DIN DIN 17155 DIN 17155 HI DIN 17155 HII DIN 17155 10CrMo910 DIN 17155 13CrMo44
DIN 17155 15Mo3 DIN 17155 17Mn4 DIN 17155 19Mn6