Nan GNEE, nou fyè dèske nou bay bon kalite- EN 10028-2 P355GH plak asye, yon asye ki pa-alyaj ki fèt pou veso presyon ak chodyè opere nan tanperati ki wo.
GNEE bay yon analiz teknik detaye sou laP355GH chodyè asye plak, konsantre sou konpozisyon chimik li yo, pwopriyete mekanik, ak konfòmite ak estanda EN 10028-2. Pou espesifikasyon konplè, al gade nan detay plak asye EN 10028-2 P355GH.
EN10028-2 P355GH presyon veso ak chodyè asye plak konpozisyon chimik ak pwopriyete mekanik
|
Klas |
Konpozisyon chimik (%) |
||||
|
C |
Mn |
Si max |
P max |
S max |
|
|
EN10028-2 P355GH |
0.1-0.22 |
1.1-1.7 |
0.6 |
0.025 |
0.015 |
|
Klas |
Pwopriyete mekanik |
|
|||
|
Fòs rupture (MPa) |
Sede fòs (MPa) min |
% elongasyon nan 2 pous (50mm) min |
Konsekans Tanperati Tès (degre) |
|
|
|
EN10028-2 P355GH |
470-650 |
355 |
20 |
+20,0,-20 |
|
EN10028-2 P355GH presyon veso ak chodyè asye plak aplikasyon
EN10028-2 P355GH presyon veso ak chodyè asye plak yo itilize nan veso presyon, chodyè, tank depo ak echanjeur chalè nan lwil oliv, pwojè gaz.
EN10028-2 P355GH Presyon Veso ak Chodyè Steel Plak Lòt Non
EN10028-2 P355GH chodyè asye plak, EN10028-2 P355GH presyon veso asye plak, EN10028-2 P355GH Depo tank asye plak. EN10028-2 P355GH Chalè echanjeur Steel Plak.
Klas asye ekivalan ak espesifikasyon pou EN 10028-2 P355GH
|
Kategori |
Detay yo |
Nòt |
|
Estanda |
EN 10028-2 P355GH |
Ranplase estanda 1501-161-360A ak DIN H 1. |
|
Klas ekivalan |
||
|
Ewòp |
Fe E355 |
Komen Ewopeyen estriktirèl ekivalan asye. |
|
Bèljik |
D52-1,2 |
Itilize nan aplikasyon pou veso presyon. |
|
Almay |
19Mn8 |
Konparab pou pèfòmans tanperati ki wo-. |
|
Lafrans |
A52 CP |
Apwopriye pou veso presyon nan estanda franse. |
|
Itali |
Fe510-1-KW |
Itilize nan chodyè Italyen ak estanda veso presyon. |
|
Syèd |
SS 21,06,01 |
Syèd ekivalan pou aplikasyon pou tanperati ki wo-. |
|
Japon |
SPV355 |
JIS estanda ekivalan pou veso presyon. |
en 10028-2 P355GH Espesifikasyon
|
||
|
Epesè |
6 mm a 300 mm |
Gwo ranje pou veso presyon, chodyèr, ak sistèm kanalizasyon. |
|
Lajè |
1500 mm a 4050 mm |
Akomode gwo -fabwikasyon. |
|
Longè |
3000 mm pou 15000 mm |
Longè fleksib pou bezwen espesifik-pwojè yo. |
|
Fòm |
Plak |
Prensipalman apwovizyone kòm plak plat; koutim koupe disponib. |
|
Tès siplemantè |
Tès HIC (NACE MR0175), Z15, Z25, Z35, S1, S2, S3, S4.1, S5, S6, S7, S8, S9, S11, S12, S14, S17 |
Asire bon jan kalite pou sèvis asid ak anviwònman presyon wo-. |
|
Kondisyon livrezon |
Nòmalize oswa kòm -woule |
Nòmalize pou ranfòse rezistans ak inifòmite. |
Nòt:
LaEN 10028-2 P355GH plak asyefèt pou pèfòmans tanperati ki wo - (jiska ~ 400 degre), ak ekselan soudabilite ak rezistans HIC, jan yo detaye nan estanda EN 10028-2 P355GH.
Klas ekivalan tankou Fe E355, SPV355, ak 19Mn8 yo chwazi baze sou pwopriyete mekanik menm jan ak aplikasyon, menm si ti varyasyon nan alyaj ka egziste.
GNEE ofriP355GH chodyè asye plaknan yon pakèt dimansyon pou satisfè espesifikasyon kliyan yo, ak tès siplemantè (egzanp, NACE MR0175 pou HIC) asire konvnab pou anviwònman sèvis tounen.
Gwosè koutim ak sètifikasyon adisyonèl disponib sou demann pou sipòte divès kondisyon pwojè.
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com.Nou plis ke kontan ede ou.



| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Class3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||