DNV F690 plak asye

Oct 20, 2025 Kite yon mesaj

DNV Klas F690, NV F690, DNV F690 plak asye posede fòs nan rupture ki pi wo nan 770-940 Mpa, ak pwen an sede minimòm yo dwe 690 Mpa. Klas F690 endike tès la enpak tanperati ki ba dwe fè anba mwens 60 santigre.

 

Estanda Steel: DNV (Det Norske Veritas)

Kalite woule: plak bato ki gen anpil fòs

Epesè: 6mm-250mm

Lajè: 1500mm-4200mm

Longè: 3000mm-18000mm

Tretman chalè: trempe ak apeze

 

Konpozisyon chimik

 

DNV F690 siplemantè segondè fòs chimik konpozisyon

Klas

Eleman Max (%)

C

Si

Mn

P

S

Al

N

DNV F690

0.18

0.10-0.55

1.6

0.025

0.025

0.015-0.08

0.020

Nb

V

Ti

Cu

B

Ni

Mo

0.02-0.05

0.04-0.10

0.02

 

0.005

 

 

 

Pwopriyete mekanik

 

DNV F690 siplemantè segondè pwopriyete jeneral fòs

Klas

 

Pwopriyete mekanik

Tès enpak Charpy V

Epesè

Sede

Tensile

Elongasyon

Degre

Enèji 1

Enèji 2

DNV F690

mm

Min Mpa

Mpa

% min

-60

J

J

t Mwens pase oswa egal a 50

690

770-940

14%

46

69

50<t Mwens pase oswa egal a 70

690

770-940

14%

46

69

70<t Mwens pase oswa egal a 150

690

770-940

14%

46

69

Remak: Enèji 1 se tès enpak transverse, Enèji 2 se longitudinal