S355ML vs S355NL se yon konparezon komen nan seleksyon asye estriktirèl, kòm tou de klas yo wo -fòs, ba- asye alyaj anba estanda EN 10025 men diferan nan pwosesis ak pèfòmans. S355NL, ki espesifye anba EN 10025 -3, se yon asye nòmalize amann, pandan y ap S355ML, anba EN 10025-4, se thermomechanically woule (TMCP).
S355NL (EN 10025-3)
S355NL se yon asye estriktirèl nòmalize oswa nòmalize woule amann-ki gen:
S: estriktirèl asye.
355: Fòs sede minimòm de 355 MPa (mwens pase oswa egal a 16 mm).
NL: Nòmalize, ak rezistans enpak teste nan -50 degre pou aplikasyon pou ba-tanperati.
Pwosesis nòmalizasyon li asire yon mikwostrikti rafine, ideyal pou klima frèt tankou platfòm lanmè.
S355ML (EN 10025-4)
S355ML se yon asye estriktirèl amann -woule thermomechanically (TMCP) ak:
S: estriktirèl asye.
355: Fòs sede minimòm de 355 MPa (mwens pase oswa egal a 16 mm).
ML: Thermomechanically woule, ak rezistans enpak teste nan -50 degre.
TMCP pwodui pi rafine grenn, amelyore fòs ak soudabilite, souvan nan yon pri ki pi ba pase nòmalizasyon.
Konparezon Chimik Konpozisyon
|
Eleman |
S355NL (EN 10025-3, Louch, max %) |
S355ML (EN 10025-4, Louch, max %) |
|---|---|---|
|
Kabòn (C) |
0.18 |
0.14 |
|
Silisyòm (Si) |
0.50 |
0.50 |
|
Manganèz (Mn) |
0.90-1.65 |
1.60 |
|
Fosfò (P) |
0.025 |
0.025 |
|
Souf (S) |
0.015 |
0.020 |
|
Azòt (N) |
0.015 |
0.015 |
|
Aliminyòm (Al) |
0.02 (min, total) |
0.02 (min, total) |
|
Niobyòm (Nb) |
0.05 |
0.05 |
|
Vanadyòm (V) |
0.12 |
0.10 |
|
Titàn (Ti) |
0.05 |
0.05 |
|
Kwòm (Cr) |
0.30 |
0.30 |
|
Nikèl (Ni) |
0.30 |
0.30 |
|
Molybdène (Mo) |
0.10 |
0.20 |
|
Kwiv (Cu) |
0.55 |
0.55 |
Konparezon pwopriyete mekanik
|
Pwopriyete |
S355NL (EN 10025-3) |
S355ML (EN 10025-4) |
|---|---|---|
|
Fòs Sede (min, MPa) |
||
|
Mwens pase oswa egal a 16 mm |
355 |
355 |
|
16 |
345 |
355 |
|
40 |
335 |
345 |
|
Fòs rupture (MPa) |
470-630 |
450-610 |
|
elongasyon (min, %) |
22 (mwens pase oswa egal a 63 mm) |
22 (mwens pase oswa egal a 40 mm) |
|
Enèji enpak (min, J) |
27 @ -50 degre (longitudinal) |
27 @ -50 degre (longitudinal) |
Soudi ak Tretman Chalè
S355NL: CEV ≤0.43% supports GMAW or SAW (EN 1011-2). Preheating (100-150°C) for >20 mm; PWHT (550-650 degre) opsyonèl. Consommables: ER70S-6 (GMAW), EM12K flux ak fil EH14 (SAW).
S355ML: Lower CEV (≤0.39%) enhances weldability, often requiring less preheating (50-100°C for >20 mm). Menm consommables aplike.
Konparezon soude S355NL ak S355ML an favè S355ML pou pri -fabwikasyon efikas akòz pwosesis TMCP li yo.
Aplikasyon
S355NL:
Platfòm lanmè nan anviwònman maren frèt.
Gwo fò won van nan klima anba-zewo.
Pon ak trepye nan rejyon nò yo.
Nòmalizasyon li asire fyab nan yon seri epesè lajè (jiska 250 mm).
S355ML:
Aplikasyon ki sanble (bò rivaj, gwo fò won van, pon) men pi pito nan pwojè priyorite soudabilite ak pri.
Limite nan seksyon mens (mwens pase oswa egal a 120 mm), apwopriye pou estrikti pi lejè.
Diferans aplikasyon S355ML S355NL a mete aksan sou adaptabilite S355NL pou plak ki pi epè ak pri -efikasite S355ML pou plak ki pi mens.