S275N ak S355N se estanda Ewopeyen an (EN 10025-3) asye estriktirèl amann-, diferansye sitou pa fòs sede (S275 gen ~ 275 MPa, S355 gen ~ 355 MPa), ak S355 ofri pi gwo fòs pou lou-pou aplikasyon pou gwo{-2 devwa, pandan y ap sèvi ak aplikasyon pou pon yo ak devwa jeneral 75 presye pou bon soudabilite ak rezistans ba-tanperati akòz deziyasyon 'N' (Nòmalize), ki fè yo versatile pou pwojè mande.
S275N ak S355N yo tou de se plak asye estriktirèl nòmalize amann-ki fèt pou konstriksyon soude ki mande pou ranfòse rezistans nan tanperati ki ba jiska -20 degre.
S275N ofri yon fòs sede minimòm de 275 MPa, pandan y ap S355N bay pi wo fòs nan 355 MPa, ki fè S355N pi apwopriye pou chaj pi lou pase S275N.
Konparezon Chimik Konpozisyon
|
Eleman |
Senbòl |
S275N Max (%) |
S355N Max (%) |
|---|---|---|---|
|
Kabòn |
C |
0.20 |
0.20 |
|
Silisyòm |
Si |
0.40 |
0.50 |
|
Manganèz |
Mn |
0.80–1.60 |
0.90–1.60 |
|
Fosfò |
P |
0.035 |
0.025 |
|
Souf |
S |
0.030 |
0.020 |
|
Kwòm |
Kr |
0.30 |
0.30 |
|
Molybdène |
Mo |
0.10 |
0.10 |
|
Vanadyòm |
V |
0.05 |
0.12 |
|
Azòt |
N |
0.012 |
0.015 |
|
Niobyòm |
Nb |
0.050 |
0.050 |
|
Titàn |
Ti |
0.050 |
0.050 |
|
Aliminyòm |
Al |
Pi gran pase oswa egal a 0.020 |
Pi gran pase oswa egal a 0.020 |
|
Kwiv |
Cu |
0.35 |
0.55 |
|
CEV |
- |
0.40 |
0.43 |
Konparezon pwopriyete mekanik
|
Epesè nominal (mm) |
Sede ReH Min (MPa) S275N |
Sede ReH Min (MPa) S355N |
Tensile Rm (MPa) S275N |
Tensile Rm (MPa) S355N |
Elongasyon A Min (%) Tou de |
Charpy KV Longitudinal Min (J) nan -20 degre Tou de |
|---|---|---|---|---|---|---|
|
Mwens pase oswa egal a 16 |
275 |
355 |
370–530 |
470–630 |
23 |
47 |
|
16 < t Mwens pase oswa egal a 40 |
265 |
345 |
370–530 |
470–630 |
23 |
47 |
|
40 < t Mwens pase oswa egal a 63 |
255 |
335 |
370–530 |
470–630 |
23 |
47 |
|
63 < t Mwens pase oswa egal a 80 |
245 |
325 |
370–530 |
470–630 |
22 |
47 |
|
80 < t Mwens pase oswa egal a 100 |
235 |
315 |
370–530 |
470–630 |
22 |
47 |
|
100 < t Mwens pase oswa egal a 150 |
225 |
295 |
350–510 |
450–600 |
22 |
47 |
|
150 < t Mwens pase oswa egal a 200 |
215 |
285 |
350–510 |
450–600 |
22 |
47 |
|
200 < t Mwens pase oswa egal a 250 |
195 |
265 |
350–510 |
450–600 |
22 |
47 |
Tretman Chalè ak Konparezon soude
Tretman Chalè: Tou de nòmalize (+N: 880-920 degre ostenitize, lè fre) pou bon -grenn.
Soudi: Ba CEV (0.40/0.43), pa prechofe Mwens pase oswa egal a 40 mm; S355N ka bezwen plis swen pou seksyon ki pi epè.
Swiv EN 1011-2. Gangsteel optimize pou tou de.