S235J0W ak S235J2W yo tou de estanda Ewopeyen an (EN 10025-5) dezagregasyon (Corten) asye, ki ofri amelyore rezistans korozyon atmosferik, ideyal pou pon, fasad, ak konstriksyon machin san yo pa bezwen pwoteksyon sifas yo. Diferans kle a se nan tès rezistans enpak yo, ak S235J0W ki mande charpy V-enèji enpak nan 0 degre, pandan y ap S235J2W mande pou li nan -20 degre, ki endike J2W ofri pi bon pèfòmans ba-tanperati pou estrikti solid, dirab.
Konpozisyon chimik nan analiz pwodwi klas S235J0W
|
C |
Si |
Mn |
Cu |
P |
S |
Kr |
N |
|
0.16 |
0.45 |
0.15-0.70 |
0.20-0.60 |
0.040 |
0.040 |
0.35-0.85 |
0.010 |
Konpozisyon chimik nan analiz pwodwi klas S235J2W
|
C |
Si |
Mn |
Cu |
P |
S |
Kr |
N |
|
0.16 |
0.45 |
0.15-0.70 |
0.20-0.60 |
0.040 |
0.035 |
0.35-0.85 |
0.010 |
Pwopriyete mekanik nan klas S235J0W
|
Tanperati |
-20 |
-10 |
0 |
20 |
|
Tès enpak Notch. Min. enèji absòbe J |
27 |
|
Epesè nominal (mm) |
rive 16 |
16 - 40 |
40 - 63 |
63 - 80 |
80 - 100 |
100 - 150 |
|
ReH - Minimòm fòs sede (MPa) |
235 |
225 |
215 |
215 |
215 |
195 |
|
Epesè nominal (mm) |
rive 3 |
3 - 100 |
100-150 |
|
Rm -Fòs rupture (MPa) |
360-510 |
360-510 |
350-500 |
|
Epesè nominal (mm) |
Pi gran pase oswa egal a 1.5<2 |
Pi gran pase oswa egal a 2﹤2.5 |
Pi gran pase oswa egal a 2.5<3 |
Pi gran pase oswa egal a 3<40 |
Pi gran pase oswa egal a 40﹤63 |
Pi gran pase oswa egal a 6﹤100 |
Pi gran pase oswa egal a 100﹤150 |
|
A - elongasyon minimòm Lo=5,65 √ So (%) Longitudinal |
19 |
20 |
21 |
26 |
25 |
24 |
22 |
Pwopriyete mekanik nan klas S235J2W
|
Tanperati |
-20 |
-10 |
0 |
20 |
|
Tès enpak Notch. Min. enèji absòbe J |
27 |
|
Epesè nominal (mm) |
rive 16 |
16 - 40 |
40 - 63 |
63 - 80 |
80 - 100 |
100 - 150 |
|
ReH - Minimòm fòs sede (MPa) |
235 |
225 |
215 |
215 |
215 |
195 |
|
Epesè nominal (mm) |
rive 3 |
3 - 100 |
100-150 |
|
Rm -Fòs rupture (MPa) |
360-510 |
360-510 |
350-500 |
|
Epesè nominal (mm) |
Pi gran pase oswa egal a 1.5<2 |
Pi gran pase oswa egal a 2﹤2.5 |
Pi gran pase oswa egal a 2.5<3 |
Pi gran pase oswa egal a 3<40 |
Pi gran pase oswa egal a 40﹤63 |
Pi gran pase oswa egal a 6﹤100 |
Pi gran pase oswa egal a 100﹤150 |
|
A - elongasyon minimòm Lo=5,65 √ So (%) Longitudinal |
19 |
20 |
21 |
26 |
25 |
24 |
22 |
Karakteristik kle
Kalite: Ba-alyaj, dezagregasyon (Corten) asye estriktirèl.
Estanda: EN 10025-5.
Fòs Sede: Minimòm 235 MPa pou epesè jiska 16mm.
Fòs rupture: Tipikman 360-510 MPa.
Rezistans korozyon: Fòme yon kouch rouye pwoteksyon (patin).
Soudabilite: Bon soudabilite pou estrikti soude, rivete oswa boulon.
Deziyasyon "J" la: Severite enpak
J0: Endike yon minimòm Charpy V-enèji enpak 27J nan 0 degre.
J2: Endike yon minimòm Charpy V-enèji enpak 27J nan -20 degre, ki fè li pi difisil nan kondisyon ki pi frèt.
Aplikasyon
Pon, fasad, gwo fò tou won, ak estrikti achitekti.
Konstriksyon machin ak tren.
Kontenè ak estrikti maren (kote pwopriyete -rouye yo dezirab).