Diferans ant P265GH ak P295GH

Dec 15, 2025 Kite yon mesaj

P265GH ak P295GH yo tou de estanda Ewopeyen an (EN 10028-2) soude, asye ki pa alyaj pou veso presyon, men diferans prensipal la chita nan yo.fòs: P295GH ofri yon pi wo fòs sede minimòm (apeprè 295 MPa) pase P265GH (apeprè 265 MPa) nan tanperati chanm, ki fè P295GH pi fò ak apwopriye pou kondisyon yon ti kras pi egzijan, menm si tou de yo fèt pou tanperati ki wo. Yo pataje aplikasyon ki sanble nan chodyèr, veso presyon, ak echanjeur chalè, men P295GH bay pi bon pèfòmans mekanik, souvan lyen ak ASTM A516 Gr. 70, pandan y ap P265GH gen rapò ak ASTM A516 Gr. 60.

 

Pwopriyete mekanik nan EN 10028 - P265GH

 

Klas

Kalite

Epesè
(mm)

Sede fòs
MPa (min)

Fòs rupture
MPa

Elongasyon
% (min)

Enèji enpak
(KV J) (min)

-20 degre

0 degre

+20 degre

P265GH

Nòmalize

Mwens pase oswa egal a 16

265

410 a 530

22

27

34

40

 

 

16>a mwens pase oswa egal a 40

255

410 a 530

22

27

34

40

 

 

40>a mwens pase oswa egal a 60

245

410 a 530

22

27

34

40

 

 

60>a mwens pase oswa egal a 100

215

410 a 530

22

27

34

40

 

 

100>a mwens pase oswa egal a 150

200

400 a 530

22

27

34

40

 

 

150>a mwens pase oswa egal a 250

185

390 a 530

22

27

34

40


Pwopriyete mekanik nan EN 10028 - P295GH

 

Kalite Epesè (mm) Sede fòs
MPa (min)
Fòs rupture
MPa
Elongasyon
% (min)
Enèji enpak
(KV J) (min)
          -20 degre 0 degre +20 degre
Nòmalize Mwens pase oswa egal a 16



 
295 460 - 580 21 27 34 40
  16>a mwens pase oswa egal a 40 290 460 - 580 21 27 34 40
  40>a mwens pase oswa egal a 60 285 460 - 580 21 27 34 40
  60>a mwens pase oswa egal a 100 260 460 - 580 21 27 34 40
  100>a mwens pase oswa egal a 150 235 440 - 570 21 27 34 40
  150>a mwens pase oswa egal a 250 220 430 - 570 21 27 34 40

 

 

Konpozisyon chimik EN 10028 P265GH

 

Eleman

% pa mas

Eleman

% pa mas

Kabòn (C)

Mwens pase oswa egal a 0.20

Silisyòm (Si)

Mwens pase oswa egal a 0.40

Manganèz (Mn)

0.80 a 1.40

Fosfò (P) (max)

0.025

Souf (S) (max)

0.015

Aliminyòm (Al)

Mwens pase oswa egal a 0.020

Azòt (N)

Mwens pase oswa egal a 0.012

Kwòm (Cr)

Mwens pase oswa egal a 0.30

Kwiv (Cu)

Mwens pase oswa egal a 0.30

Molybdène (Mo)

Mwens pase oswa egal a 0.08

Niobyòm (Nb)

Mwens pase oswa egal a 0.020

Nikèl (Ni)

Mwens pase oswa egal a 0.30

Titàn (Ti) (max)

0.03

Vanadyòm (V)

Mwens pase oswa egal a 0.02

 

Konpozisyon chimik nan EN 10028 - P295GH

 

C 0.08 a 0.20
Si Mwens pase oswa egal a 0.40
Mn 0.90 a 1.50
P 0.025
S 0.015
Al Mwens pase oswa egal a 0.020
N Mwens pase oswa egal a 0.012
Kr Mwens pase oswa egal a 0.30
Cu Mwens pase oswa egal a 0.30
Mo Mwens pase oswa egal a 0.08
Nb Mwens pase oswa egal a 0.020
Ni Mwens pase oswa egal a 0.30
Ti 0.03
Vi Mwens pase oswa egal a 0.02

 

Aplikasyon

P265GH Aplikasyon tipik:

Veso presyon ki ba ak mwayen

Echanjeur chalè

Tank depo

Eleman chofaj

Aplikasyon ki mande pi bon fòmabilite

P295GH Aplikasyon tipik:

Pi wo -veso presyon

Ekipman pwosesis

Konpozan jenerasyon pouvwa

Aplikasyon kote pi wo fòs pèmèt rediksyon pwa

Konsiderasyon Seleksyon:

Chwazi P265GH lè pi bon fòmabilite oswa rezistans tanperati ki ba -

Chwazi P295GH pou aplikasyon pou presyon ki pi wo oswa kote rediksyon pwa priyorite

Konsidere P295GH pou aplikasyon pou kote yon ti kras pi wo rezistans tanperati ki nesesè

Evalye kondisyon soude, kòm P265GH jeneralman ofri pi bon soudabilite