ASTM A285 Steel Entwodiksyon:
ASTM A285 se yon kalite asye kabòn òdinè ki fèt pou fizyon -soude ekipman veso presyon kòm chodyè, tank depo, echanjeur chalè, elatriye. Avèk 3 klas asye (Klas A, Klas B, Klas C) ki kouvri ranje fòs rupture soti nan 310 -515Mpa, anjeneral ASTM A285 plak {8} te delivre kòm plak asye {8} woule. fèt pa touye, semi-touye, capped oswa rimmed pratik asye dapre egzijans itilizatè yo.
ASTM A285 asye ta ka fabrike nan anpil fòm pwodwi asye, plak asye, bobin asye, tiyo asye, li gen bon soude -kapasite pou bezwen soude fizyon pou ekipman veso presyon, epesè max li limite a 50mm yo nan lòd yo asire pwopriyete mekanik li yo.

 

ASTM A283 Steel Entwodiksyon:
ASTM A283 fèt kòm yon kalite plak asye kabòn pou objektif jeneral estriktirèl, asye sa a gen fòs rupture ki ba ak entèmedyè, li gen 2 klas asye (Klas C, Klas D). Pou plak asye ki fèt ak bobin oswa ki pa gen okenn tretman chalè, se tès adisyonèl obligatwa pou soulaje estrès li yo, anjeneral apre bobin asye yo dekole, enspeksyon, kondisyone, tretman chalè yo mande anvan livrezon. ASTM A283 se sèlman itilize pou objektif estriktirèl, pandan y ap ASME SA283 / SA283M plak asye ta ka itilize tou nan chodyè ak fabrike veso presyon.

 

Konpozisyon chimik ASTM A285:

ASTM A285 konpozisyon chimik Klas A Klas B Klas C
Kabòn, max 0.17 0.22 0.28
Manganèz, max 0.90 0.90 0.90
Fosfò, max 0.035 0.035 0.035
Souf, max 0.035 0.035 0.035

 

Konpozisyon chimik ASTM A283:

ASTM A283 Eleman chimik (max) Analiz Chalè, %
Klas C Klas D
Kabòn 0.24 0.27
Manganèz 0.90 0.90
Fosfò 0.030 0.30
Souf 0.030 0.030
Silisyòm    
Plak 11⁄2 pous [40 mm] ak anba, max 0.40 0.40
Plak plis pase 11⁄2 pous [40 mm] 0.15-0.40 0.15-0.40
Kwiv 0.20 0.20

 

Konparezon pwopriyete mekanik ASTM A283 ak ASTM A285

Konparezon pwopriyete mekanik ASTM A283 ak ASTM A285
Steel Klas Fòs rupture ,min Ksi Mpa Fòs sede min Ksi Mpa Elongasyon nan 2 pous
(50 mm)% min.
ASTM A-36 / A-36 M 58-80 ( 400-550 ) 36 ( 250 ) 23
ASTM A-283 / A-283 M gr A 45-60 ( 310-415 ) 24 ( 165 ) 30
ASTM A-283 / A-283 M gr B 50-65 ( 345-450 ) 27 ( 215 ) 28
ASTM A-283 / A-283 M gr C 55-75 ( 380-515 ) 30 ( 205 ) 25
ASTM A-283 / A-283 M gr D 60-80 ( 415-550 ) 33 ( 230 ) 23
ASTM A-285 / A-285 M gr A 45-65 ( 310-450 ) 24 ( 165 ) 30
ASTM A-285 / A-285 M gr B 50-70 ( 345-485 ) 27 ( 215 ) 28
ASTM A-285 / A-285 M gr C 55-75 ( 380-515 ) 30 ( 205 ) 27

 

A283 se yon jeneral ki ba/entèmedyè fòs estriktirèl asye, pandan y ap A285 se espesyalman pou fizyon -soude veso presyon, ofri pi bon pèfòmans segondè -tanperati (jiska 900 degre F kont {. 650 degre F pou A283) ak klas fòs menm jan an (A, B, C), fè A285 tank siperyè pou chodyèr. Diferans kle yo se nan itilizasyon entansyon yo (estriktirèl kont veso presyon), kontwòl konpozisyon chimik, ak tanperati sèvis maksimòm, ak klas A285 (A, B, C) jeneralman gen yon ti kras pi bon duktilite.