Corten B Weather Resistant Steel Plak yo itilize nan machin, pon, gwo kay won, veso ak sou sa.
Corten B Tan Rezistan Steel Plak Lòt Non
Corten B Tan Rezistan Steel plak, Corten B Tan Rezistan Steel Plak, Corten B Tan Rezistan Fèy Steel, Corten B Tan Rezistan Fèy Steel.
Kondisyon adisyonèl
UT (Egzamen Ultrasonic), AR (Kòm woule cho sèlman), TMCP (Tèmik Pwosesis kontwòl mekanik), N (Normalize), Q + T (Tenn ak Tanperaman), Tès Direksyon Z (Z15, Z25, Z35), Tès Enpak Charpy V - Notch, Tès Twazyèm Pati (tankou Tès SGS), kouvwi ak pating.
|
Corten BKonpozisyon chimik |
|||||
|
Klas |
Eleman Max (%) |
||||
|
C |
Si |
Mn |
P |
S |
|
|
Corten B |
0.19 |
0.30-0.65 |
0.80-1.25 |
0.035 |
0.030 |
Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
Klas |
|
Corten BPwopriyete mekanik |
||
|
Epesè |
Sede |
Tensile |
Elongasyon |
|
|
Corten B |
mm |
Min Mpa |
Mpa |
% min |
|
6-40 |
345 |
485 |
19 |
|