Pwopriyete chimik SB450 chodyè bon jan kalite asye

 

SB480 chodyè asye plak se yon plak asye wo-pèfòmans pou chodyèr ak veso presyon, ak yon pakèt aplikasyon ak karakteristik pèfòmans ekselan.

 

SB480 chodyè asye gen gwo estabilite tèmik epi li fasil pou trete tankou koupe, koube, ak soude. Li apwopriye pou divès kalite ekipman wo-tanperati.

 

SB480 presyon veso bon jan kalite asye analiz chimik

Klas C. % Mn.% S. N Cu Nb Ti. Si. P. AL Kr. Mo. Ni Vi
SB480 0.10-0.22 0.10-1.70 0.015 0.012 0.30 0.020 0.03 0.60 0.025 0.020 0.30 0.08 0.30 0.02

 

SB480 chofaj asye mekanik pwopriyete

Klas Epesè mm Fòs sede Mpa (min) Fòs rupture MPa Elongasyon % (min) Enèji enpak (KVJ) (min)
-20 degre 0 degre +20
SB480

Mwens pase oswa egal a 16

16 > nan mwens pase oswa egal a 40

40 > a mwens pase oswa egal a 60

60 > a mwens pase oswa egal a 100

100 > a mwens pase oswa egal a 150

150 > a mwens pase oswa egal a 250

355 510-650 20 27 34 40
345 510-650 20 27 34 40
335 460-580 20 27 34 40
315 490-630 20 27 34 40
295 480-630 20 27 34 40
280 470-630 20 27 34 40

 

PVQ Steel Plate