ASTM A537 Klas 3 Steel Plak

Sep 25, 2025 Kite yon mesaj

A537CL3, A537 Klas 3, A537CL3 plak asye yo trempe ak tanperaman kabòn Manganèz Silisyòm asye plak fèt pou fizyon veso presyon soude ak estrikti.

 

Steel Creole: ASTM A537/A537M

Kalite woule: plak asye chodyè, plak asye veso presyon

Epesè: 6mm-300mm

Lajè: 1500mm-4200mm

Longè: 3000mm-18000mm

Tretman chalè: trempe ak apeze

 

A537 klas 3Konpozisyon chimik

A537 klas 3Konpozisyon chimik

Klas

Eleman Max (%)

C

Mn

P

S

Si

Cu

Ni

Kr

Mo

A537 klas 3

0.24

0.92-1.72

0.035

0.035

0.13-0.55

0.38

0.28

0.29

0.09

Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

A537 klas 3 Pwopriyete mekanik

Klas

A537 klas 3 Pwopriyete mekanik

Epesè

Sede

Tensile

Elongasyon

A537 klas 3

mm

Min Mpa

Mpa

% min

-65

380

550-690

22

65-100

345

515-655

20

100-150

275

485-620

-

 

ASTM A537 klas 3 (A537CL3) veso presyon ak chodyè asye plak lòt non

ASTM A537 Klas 3 (A537CL3) Chodyè asye plak, ASTM A537 Klas 3 (A537CL3) Presyon Veso Steel plak, ASTM A537 Klas 3 (A537CL3) Tank Depo Steel plak. ASTM A537 klas 3 (A537CL3) chalè echanjeur asye plak .

 

Kondisyon adisyonèl

UT (Egzamen Ultrasonic), AR (Kòm woule cho sèlman), TMCP (Tèmik Pwosesis kontwòl mekanik), N (Normalize), Q + T (Tenn ak Tanperaman), Tès Direksyon Z (Z15, Z25, Z35), Tès Enpak Charpy V - Notch, Tès Twazyèm Pati (tankou Tès SGS), kouvwi ak pating.