ASTM A302 Klas B plak asye alyaj pou veso presyon

Nov 10, 2025 Kite yon mesaj

GNEE founi ASTM A302Gr.B plak asye ak A302 Klas B presyon veso asye plak. ASTM A302GRB se manganèz -molybdène- nikèl alyaj plak asye.

  • Mo kle: ASTM A302GR.B, A302 Klas B, A302 Gr.B plak asye, ASTM A302GrB plak asye
  • Adopte estanda: A 302/A 302M-03
  • Vann klas asye: A302 Klas A, A302 Klas B, A302 Klas C, A302 Klas D klas asye

A302 GrB Pressure Vessel Steel Plate

A302 Klas B plak asye spesifikasyon estanda pou plak veso presyon nan asye alyaj, manganèz molybdène ak manganèz -molybdène- nikèl.

 

A302 Klas B klas asye se min fòs sede nan 310Mpa. GNEE tou bay tès la ultrasons nan epesè nan A435 / A435M, A577 / 577M ak A578 / A578M pwomèt bon jan kalite a pafè nan koperasyon long.

 

Plak asye A302 Klas B yo dwe nòmalman apwovizyone nan kondisyon kòm -woule. Plak yo ka kòmande nòmalize oswa soulaje estrès, oswa toude. Si plak asye A302 Klas B pi wo pase 50mm nan epesè yo pral nòmalize.

 

A302 Klas B chodyè ak presyon veso asye konpozisyon chimik ak pwopriyete mekanik

 

Klas A302 klas B asye konpozisyon chimik (%)
C Mn Greater than or equal to Si P S
ASTM A302 Klas B (A302GRB) 0.2 1.07-1.62 0.13-0.45 0.035 0.035
Klas A302 Klas B asye Pwopriyete mekanik
Fòs rupture (MPa) Sede fòs (MPa) % elongasyon nan 2 pous (50mm) min Konsekans Tanperati Tès (degre)
ASTM A302 Klas B (A302GRB) 550-690 345 20 -20,40,-60

 

Nwayo pèfòmans Avantaj nan A302 GrB presyon veso Steel Plak

 

A302 GrB Pressure Vessel Steel PlateEkselan -Direte tanperati ki ba
Plak asye alyaj A302 GrB fèt pou fè byen nan anviwònman tanperati ki ba -. Sa a se youn nan rezon prensipal li lajman itilize nan aplikasyon pou veso presyon ki enplike kondisyon kriyojenik. Plak asye a kenbe severite li yo ak rezistans enpak menm nan tanperati osi ba ke -40 degre, sa ki fè li yon chwa ideyal pou tank depo ba-tanperati ak veso presyon.

 

Segondè fòs ak rezistans
A302 GrB plak asye woule cho gen gwo fòs rupture, ki fè li apwopriye pou anviwònman presyon wo -. Kapasite materyèl la pou kenbe tèt ak kondisyon presyon ekstrèm san echèk esansyèl nan endistri tankou jenerasyon pouvwa ak pwodiksyon pétrochimique, kote veso presyon yo ekspoze a gwo estrès entèn yo.

 

A302 GrB Pressure Vessel Steel PlateRezistans korozyon
A302 GrB presyon veso asye plak ofri bon rezistans nan korozyon atmosferik, espesyalman lè ekspoze a anviwònman modere. Li kapab manyen ekspoze modere nan sibstans ki sou korozivite, fè li apwopriye pou itilize nan pwosesis chimik ak endistri petwochimik.

 

Pri-Efikasite ak Disponibilite
Plak asye chodyè A302 GrB gen yon pri ki pi ba pase kèk asye alyaj ki wo -, tankou 9% asye nikèl oswa segondè- asye pur. Sa fè li yon chwa pri-efikas pou aplikasyon kote pèfòmans ekstrèm materyèl alyaj ki pi wo-pa nesesè.

 

Mande Yon Quote

 

Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.

 

Klas Plak Veso Presyon Apwovizyone Pa GNEE
ASTM ASTM A202/A202M ASTM A202 Klas A ASTM A202 Klas B    
ASTM A203/A203M ASTM A203 Klas A ASTM A203 Klas B ASTM A203 Klas D ASTM A203 Klas E
ASTM A203 Klas F      
ASTM A204/A204M ASTM A204 Klas A ASTM A204 Klas B ASTM A204 Klas C  
ASTM A285/A285M ASTM A285 Klas A ASTM A285 Klas B ASTM A285 Klas C  
ASTM A299/A299M ASTM A299 Klas A ASTM A299 Klas B    
ASTM A302/A302M ASTM A302 Klas A ASTM A302 Klas B ASTM A302 Klas C ASTM A302 Klas D
ASTM A387/A387M ASTM A387 Klas 5 Klas1 ASTM A387 Klas 5 Klas2 ASTM A387 Klas 11 Klas1 ASTM A387 Klas 11 Klas2
ASTM A387 Klas 12 Klas1 ASTM A387 Klas 12 Klas2 ASTM A387 Klas 22 Klas1 ASTM A387 Klas 22 Klas2
ASTM A515/A515M ASTM A515 Klas 60 ASTM A515 Klas 65 ASTM A515 Klas 70  
ASTM A516/A516M ASTM A516 Klas 55 ASTM A516 Klas 60 ASTM A516 Klas 65 ASTM A516 Klas 70
ASTM A517/A517M ASTM A517 Klas A ASTM A517 Klas B ASTM A517 Klas E ASTM A517 Klas F
ASTM A517 Klas P ASTM A517 klas J    
ASTM A533/A533M ASTM A533 Klas A Klas 1 ASTM A533 Klas B Klas1 ASTM A533 Klas C Class1 ASTM A533 Klas D Class1
ASTM A533 Klas A Klas2 ASTM A533 Klas B Klas2 ASTM A533 Klas C Class2 ASTM A533 Klas D Klas2
ASTM A533 Klas A Klas3 ASTM A533 Klas B Klas3 ASTM A533 Klas C Class3 ASTM A533 Klas D Class3
ASTM A537/A537M ASTM A537 Klas 1 ASTM A537 Klas 2 ASTM A537 Klas 3  
ASTM A612/A612M ASTM A612      
ASTM A662/A662M ASTM A662 Klas A ASTM A662 Klas B ASTM A662 Klas C  
EN EN10028-2 EN10028-2 P235GH EN10028-2 P265GH EN10028-2 P295GH EN10028-2 P355GH
EN10028-2 16MO3      
EN10028-3 EN10028-3 P275N EN10028-3 P275NH EN10028-3 P275NL1 EN10028-3 P275NL2
EN10028-3 P355N EN10028-3 P355NH EN10028-3 P355NL1 EN10028-3 P355NL2
EN10028-3 P460N EN10028-3 P460NH EN10028-3 P460NL1 EN10028-3 P460NL2
EN10028-5 EN10028-5 P355M EN10028-5 P355ML1 EN10028-5 P355ML2 EN10028-5 P420M
EN10028-5 P420ML1 EN10028-5 P420ML2 EN10028-5 P460M EN10028-5 P460ML1
EN10028-5 P460ML2      
EN10028-6 EN10028-6 P355Q EN10028-6 P460Q EN10028-6 P500Q EN10028-6 P690Q
EN10028-6 P355QH EN10028-6 P460QH EN10028-6 P500QH EN10028-6 P690QH
EN10028-6 P355QL1 EN10028-6 P460QL1 EN10028-6 P500QL1 EN10028-6 P690QL1
EN10028-6 P355QL2 EN10028-6 P460QL2 EN10028-6 P500QL2 EN10028-6 P690QL2
JIS JIS G3115 JIS G3115 SPV235 JIS G3115 SPV315 JIS G3115 SPV355 JIS G3115 SPV410
JIS G3115 SPV450 JIS G3115 SPV490    
JIS G3103 JIS G3103 SB410 JIS G3103 SB450 JIS G3103 SB480 JIS G3103 SB450M
JIS G3103 SB480M      
GB GB713 GB713 Q245R GB713 Q345R GB713 Q370R GB713 12Cr1MoVR
GB713 12Cr2Mo1R GB713 13MnNiMoR GB713 14Cr1MoR GB713 15CrMoR
GB713 18MnMoNbR      
GB3531 GB3531 09MnNiDR GB3531 15MnNiDR GB3531 16MnDR  
DIN DIN 17155 DIN 17155 HI DIN 17155 HII DIN 17155 10CrMo910 DIN 17155 13CrMo44
DIN 17155 15Mo3 DIN 17155 17Mn4 DIN 17155 19Mn6