Plak asye SA302GrB se yon sèl kalite asye alyaj Molybdène nan ASME SA302 / SA302M, SA302 Klas B totalman egal aA302 Klas Bnan ASTM A302 / A302 spesifikasyon asye.Sepandan ki klas asye nan spesifikasyon asye Chinwa ki ekivalan a SA302 Klas B plak asye?
Konparasyon pwopriyete mekanik ak konpozisyon chimik ki soti nan tablo ki anba a, nou jwenn plak asye 15CrMoR nan estanda asye GB/T713 pou chodyè bilding asye itilize trè menm jan akSA302GRB plak asye.Yo tout bezwen Mo% pi wo pase 0.45% lè yo founi ak tretman chalè ak Normalized.Else,15CrMoR plak asyegen plis restriksyon pou P% ak S% lè woule.
SA302 Klas A plak asyeitilize pou chodyèr fabrike ak veso presyon ak Mo (Min.0.45%) alloy.15CrMoR plak asye tou yo itilize pou chodyèr ak ak alyaj Mo nan 0.45-0.6% nan analiz chalè woule.
Konparasyon nan konpozisyon chimik ak fòs mekanik nan tablo anba a, nan pifò sitiyasyon, plak asye SA302 Klas A egal a plak asye 15CrMoR lè yo bati chodyèr ak veso presyon.
Konpozisyon chimik ak pwopriyete mekanik
|
SA302GrBvs15CrMoR |
Konpozisyon chimik: analiz chalè Max% |
|||||||||
|
Estanda |
Klas |
C |
Mn |
P |
S |
Si |
Cu |
Ni |
Kr |
Mo |
|
ASME SA302/SA302M |
SA302GrB |
0.20 |
0.85-1.20 |
0.025 |
0.025 |
0.15-0.40 |
- |
- |
- |
0.45-0.6 |
|
GB/T 713 |
15CrMoR |
0.08-0.18 |
1.15-1.50 |
0.025 |
0.010 |
0.15-0.40 |
0.30 |
0.30 |
0.8-1.2 |
0.45-0.6 |
|
Pwopriyete mekanik: |
Epesè |
Sede fòs |
Fòs rupture |
|||||||
|
Mpa Min. |
Mpa |
|||||||||
|
ASME SA302/SA302M |
SA302GrB |
|
345 |
550-690 |
||||||
|
GB/T 713 |
15CrMoR |
T Mwens pase oswa egal a 60 |
295 |
450-690 |
||||||
Senaryo Aplikasyon: Ekivalans nan Pratik ak Konsèy pou Seleksyon
Tou deSA302GrB presyon veso asye plakepi15CrMoR cho woule plak asyeyo lajman itilize nan chodyèr, veso presyon, ak echanjeur chalè, ak ekivalans yo valide nan anpil pwojè endistriyèl:

Aplikasyon tipik nan SA302GrB
Pwojè ki sètifye nan lòt bò dlo ASME-: Réacteurs pétrochimiques, veso pwesyon pou tretman gaz natirèl, ak tib chodyè chodyè.
Senaryo gwo-presyon, ba-tanperati: Réacteurs Idwojènasyon, ekipman oksilyè plant GNL, ak aparèy chofaj presyon wo-izin tèmik.
Avantaj: rekonesans estanda mondyal senplifye akizisyon trans--fwontyè ak sètifikasyon pwojè, sa ki fè li yon chwa prensipal pou pwojè EPC entènasyonal yo.
Aplikasyon tipik nan 15CrMoR
Domestik GB-pwojè estanda: chabon-tanbou chodyè plant elektrik, endistri chimik reyaktè sentèz metanol, ak veso presyon tretman dlo egou yo.
Anviwònman tanperati ki wo -korozif: Ekipman pwodiksyon asid silfirik, gwo fò won tretman ilfid idwojèn, ak eleman echanj chalè chodyè ensinerasyon fatra.
Avantaj: Pri -efikasite (10-15% pi ba pase SA302GrB) ak chèn ekipman domestik ki gen matirite, apwopriye pou pwojè domestik ak kontwòl pri strik.
Si ou vle aprann plis sou pwodwi GNEE yo, ou ka voye yon imèl bayalloy@gneesteelgroup.com. Nou plis ke kontan ede ou.
| Klas Plak Veso Presyon Apwovizyone Pa GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 Klas A | ASTM A202 Klas B | ||
| ASTM A203/A203M | ASTM A203 Klas A | ASTM A203 Klas B | ASTM A203 Klas D | ASTM A203 Klas E | |
| ASTM A203 Klas F | |||||
| ASTM A204/A204M | ASTM A204 Klas A | ASTM A204 Klas B | ASTM A204 Klas C | ||
| ASTM A285/A285M | ASTM A285 Klas A | ASTM A285 Klas B | ASTM A285 Klas C | ||
| ASTM A299/A299M | ASTM A299 Klas A | ASTM A299 Klas B | |||
| ASTM A302/A302M | ASTM A302 Klas A | ASTM A302 Klas B | ASTM A302 Klas C | ASTM A302 Klas D | |
| ASTM A387/A387M | ASTM A387 Klas 5 Klas1 | ASTM A387 Klas 5 Klas2 | ASTM A387 Klas 11 Klas1 | ASTM A387 Klas 11 Klas2 | |
| ASTM A387 Klas 12 Klas1 | ASTM A387 Klas 12 Klas2 | ASTM A387 Klas 22 Klas1 | ASTM A387 Klas 22 Klas2 | ||
| ASTM A515/A515M | ASTM A515 Klas 60 | ASTM A515 Klas 65 | ASTM A515 Klas 70 | ||
| ASTM A516/A516M | ASTM A516 Klas 55 | ASTM A516 Klas 60 | ASTM A516 Klas 65 | ASTM A516 Klas 70 | |
| ASTM A517/A517M | ASTM A517 Klas A | ASTM A517 Klas B | ASTM A517 Klas E | ASTM A517 Klas F | |
| ASTM A517 Klas P | ASTM A517 klas J | ||||
| ASTM A533/A533M | ASTM A533 Klas A Klas 1 | ASTM A533 Klas B Klas1 | ASTM A533 Klas C Class1 | ASTM A533 Klas D Class1 | |
| ASTM A533 Klas A Klas2 | ASTM A533 Klas B Klas2 | ASTM A533 Klas C Class2 | ASTM A533 Klas D Klas2 | ||
| ASTM A533 Klas A Klas3 | ASTM A533 Klas B Klas3 | ASTM A533 Klas C Class3 | ASTM A533 Klas D Class3 | ||
| ASTM A537/A537M | ASTM A537 Klas 1 | ASTM A537 Klas 2 | ASTM A537 Klas 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 Klas A | ASTM A662 Klas B | ASTM A662 Klas C | ||
| EN | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| EN10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||