ABS FH36 plak asye maren ki lajman ki itilize nan konstriksyon bato ak lòt estrikti maren. Biwo Ameriken pou Shipping (ABS) espesifye klas la epi yo renome pou ekselan fòs, severite, ak soudabilite yo.
|
ABS FH36 segondè fòs chimik konpozisyon |
|||||||
|
Klas |
Eleman Max (%) |
||||||
|
C |
Si |
Mn |
P |
S |
Al |
N |
|
|
ABS FH36 |
0.16 |
0.1-0.50 |
0.90-1.6 |
0.025 |
0.025 |
0.015 |
0.009 |
|
Nb |
V |
Ti |
Cu |
Kr |
Ni |
Mo |
|
|
0.02-0.05 |
0.05-0.10 |
0.02 |
0.35 |
0.2 |
0.8 |
0.08 |
|
Sansiblite krak: Pcm=(C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
|
ABS FH36 pwopriyete segondè fòs |
|||||||
|
Klas |
|
Pwopriyete mekanik |
Tès enpak Charpy V |
||||
|
Epesè |
Sede |
Tensile |
Elongasyon |
Degre |
Enèji 1 |
Enèji 2 |
|
|
ABS FH36 |
mm |
Min Mpa |
Mpa |
% min |
-60 |
J |
J |
|
t Mwens pase oswa egal a 50 |
355 |
490-620 |
21% |
24 |
34 |
||
|
50<t Mwens pase oswa egal a 70 |
355 |
490-620 |
21% |
27 |
41 |
||
|
70<t Mwens pase oswa egal a 100 |
355 |
490-620 |
21% |
34 |
50 |
||
|
Remak: Enèji 1 se tès enpak transverse, Enèji 2 se longitudinal |
|||||||
Plak asye ABS FH36 yo anjeneral apwovizyone nan yon kondisyon nòmal oswa trempe ak apeze. Tretman chalè nòmal enplike chofe asye a nan yon tanperati espesifik ak Lè sa a, pèmèt li refwadi tou dousman, ki amelyore estrikti entèn li yo ak pwopriyete mekanik. Trempe ak tanperaman asye, nan lòt men an, sibi yon pwosesis tretman chalè ki pi solid ki enplike rapid refwadisman (trempe) ki te swiv pa tanperaman pou reyalize nivo fòs ak severite vle.
Tès enpak se yon pati esansyèl nan pwosesis kontwòl kalite pou plak asye ABS FH36. Tès sa a enplike asye a anba fòs enpak tanperati ba-pou evalye solidite li ak kapasite li pou reziste anba chay toudenkou. Rezilta tès sa yo asire ke plak asye yo satisfè nòm strik yo fikse pa ABS la pou itilize nan aplikasyon maren.