ASTM A514 Klas J se yon plak asye alyaj ki trempe ak apeze pou plis fòs. Li fè pati gwoup A514, ak metal tankou nikèl ak molybdène pou fè li difisil. Estanda ASTM A514 kouvri plak asye solid pou soude nan kote difisil. Klas J se pou plak mens, ak fòs sede segondè.
Epesè: 6MM a 300MM,
Lajè: 1500mm a 4050mm,
Longè: 3000mm a 15000mm
A514 Klas J Konpozisyon Chimik
|
A514 Klas J Konpozisyon Chimik |
|||||||||||||||
|
A514 Klas J |
Eleman Max (%) |
||||||||||||||
|
C |
Mn |
P |
S |
Si |
Ni |
Kr |
Mo |
V |
Ti |
Zr |
Cu |
B |
Nb |
||
|
0.12-0.21 |
0.45-0.70 |
0.035 |
0.035 |
0.20-0.35 |
- |
- |
0.50-0.65 |
- |
- |
- |
- |
0.001-0.005 |
- |
||
Ekivalan kabòn: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A514 Klas J Pwopriyete Mekanik
|
Klas |
A514 Klas J Pwopriyete Mekanik |
|||
|
Epesè |
Sede |
Tensile |
Elongasyon |
|
|
A514 klas J |
mm |
Min Mpa |
Mpa |
% min |
|
20 |
690 |
760-895 |
18 |
|
|
20-65 |
690 |
760-895 |
18 |
|
|
65-150 |
620 |
690-895 |
18 |
|
Klas asye ekivalan nan A514 klas J
|
Klas asye ekivalan nan A514 klas J |
||
|
EN 10149-2 |
SEW 092 |
NFA 36-231 |
|
S700MC |
QStE 690 TM |
E 690 D |
Aplikasyon nan A514 Klas J Steel Plak
ASTM A514 GR J plak yo itilize nan kote ki bezwen gwo fòs nan materyèl mens. Se pou veso presyon ak tank ki kenbe presyon ki wo. Li la tou nan pati estriktirèl pou machin ak bilding.