1. Klasifikasyon ak Sistèm Creole (Enhanced)
1.1 ASTM Seri estanda
A36:
Kontni kabòn mwens pase oswa egal a 0.26%, MN: 0.60-0.90%
Ekonomik pou kolòn estriktirèl (epesè mwens pase oswa egal a 200mm)
Enpak andirans byen wo diminye anba a -30 degre
A283 Klas C:
Pou tank depo (k ap travay presyon mwens pase oswa egal a 1.6MPa)
SI kontni (0.10-0.50%) kritik pou frèt koube
AS-woule livrezon epesè: 6-40mm
A572 Klas 50:
Mikwo-alye ak 0.05% NB, sede fòs 38%> A36
Exempts PWHT pou plak mwens pase oswa egal a 100mm (egzanp, George Washington Bridge)
1.2 Estanda Ewopeyen an (EN/DIN)
S235jr:
Kondisyon livrezon make obligatwa (egzanp, "+n"=normalized)
Baltik lanmè pwojè van mande pou S235J2W (-20 degre enpak pi gran pase oswa egal a 27J)
1.3 Estanda Japonè (JIS)
SM400:
SM400A (P mwens pase oswa egal a 0.035%, s mwens pase oswa egal a 0.035%) pou sismik ki reziste jwenti (egzanp, Tokyo Bay Bridge)
1.4 Estanda Chinwa (GB)
Q235B:
Adhesion zenk dwe satisfè ASTM D3359 Klas B
Itilize nan tren Qinghai-Tibet ak dezagregasyon asye Q355NH
2. Konparezon pèfòmans kle (ogmante)
| Egalize | CE fòmil | Tan tranzisyon (degre) | Ranje travay cho (degre) |
|---|---|---|---|
| A572 Gr.50 | C+Mn/6+ Si/24 | -45 | 900–1200 |
| S235jr | C+Mn/20+ Si/30 | -20 | 850–1150 |
| Q235B | C+Mn/6+ Cr/5 | -30 | 950–1250 |
3. Gid seleksyon materyèl (pratik jeni)
3.1 Konvèsyon estanda
Pwojè Saudi Aramco: Mande siplemantè tès S-kontni lè melanje A36/S235JR
ASTM: S mwens pase oswa egal a 0.050% vs en: s mwens pase oswa egal a 0.045%
3.2 Weldability
A572 Gr.50 (pi gran pase oswa egal a 38mm): Sèvi ak AWS D1.8 Low-idwojèn elektwòd + 150 Degre Chofeat
3.3 Kondisyon Rejyonal yo
Sidès Azi: Ajoute ISO 9223 tès espre sèl nan estanda GB
4. Echèk etid ka (teknik ekstansyon)
4.1 A36 ensidan kase (Monreyal estad)
Kòz rasin: Insufficient impact testing (thickness >50mm nan tanperati anbyen)
Solisyon: Aplike ASTM A673 pran echantiyon (1 seri/15 tòn)
4.2 Q235B Weld Cracking (Baosteel Bilten teknik)
Jwenn kritik: Diminye limit CE soti nan 0.42% a 0.38% pou plak pi gran pase oswa egal a 25mm
5. Akizisyon & Kontwòl Kalite (Pwotokòl Operasyonèl)
5.1 Kondisyon Sètifikasyon
| Estanda | Dokiman obligatwa |
|---|---|
| Astm | A2LA-akredite Charpy V-Notch Rapò (3-echantiyon AVG.) |
| En | En 10204 3.2 ak Inyon Ewopeyen Notifye Kò No (egzanp, NB 2796) |
| JIS | JIS Mak via JQA/JIS-sètifye Odit faktori Anyèl |
5.2 Materyèl trasabilite
Pèmanan make: chalè pa gen okenn, estanda, klas
Tès pakèt: rupture (ASTM A370/EN ISO 6892-1), Bend, enpak
6. Kwa-estanda ekivalans
| Astm | En | JIS | GB | Kle aplikasyon |
|---|---|---|---|---|
| A36 | S235jr | SS400 | Q235B | Bati ankadreman |
| SA283 Gr.c | P275NH | SPV490 | 20R | Veso presyon<1.6MPa |
| A572 Gr.50 | S355jr | SM490 | Q355B | Bridges >Epesè 38mm |
Remak sou pwopriyete atravè-epesè:
Z35> z25> z15 pou lamèl rezistans chire
NDT Nivo: Nivo 1 (strik)> Nivo 2> Nivo 3