ASTM A 633/A633M: 2018 PDF
Espesifikasyon estanda pou plak asye estriktirèl alyaj nòmalize segondè -fòs ba-

ASTM A633/A633M-01 PDF
ASTM A633 ekivalan
Q345

ASTM A633 se yon spesifikasyon pou plak asye estriktirèl segondè -fòs ki ba-. Klas ekivalan yo enkli EStE380 ak EN 10113-3 S355ML. Pou aplikasyon espesifik, tankou sa yo ki mande pou severite dan siperyè nan tanperati ki ba, ASTM A633 Klas E se yon bon chwa.
EN 10113-3 S355ML: Yon estanda Ewopeyen ekivalan a ASTM A633.
ASTM A572 Klas 50: Gen kèk sous ki endike li ekivalan a EN S355JR, ki se yon klas ki pi ba pase A633.
ASTM A36: Yon klas asye grav komen, men se pa dirèkteman ekivalan a A633.
Konpozisyon chimik
Pwopriyete konpozisyon sa yo se espesifikasyon ASTM pou klas A633.
| Klas A | |
| Kabòn max | 0.18% |
| Manganèz | 1.00-1.35% |
| Fosfò max | 0.030% |
| Souf max | 0.030% |
| Silisyòm | 0.15-0.50% |
| Columbium | 0.05% max |
| Klas C | |
| Kabòn max | 0.20% |
| Manganèz | 1.15-1.50% |
| Fosfò max | 0.030% |
| Souf max | 0.030% |
| Silisyòm | 0.15-0.50% |
| Columbium | 0.01-0.05% |

| Klas D | |
| Kabòn max | 0.20% |
| Manganèz, Mwens pase oswa egal a 1 1/2" epè | 0.70-1.35% |
| Manganèz, Plis pase 1 1/2 "a & enkli 4" epè | 1.00-1.60% |
| Fosfò max | 0.030% |
| Souf max | 0.030% |
| Silisyòm | 0.15-0.50% |
| Copper max | 0.35% |
| Nikèl max | 0.25% |
| Kwòm max | 0.25% |
| Molybdène max | 0.08% |
ASTM A633 klas D kabòn asye plak resous stock nan Lachin:
| Klas | Epesè (mm) | Lajè (mm) | Longè (mm) |
| A633D | 126 | 2440 | 5250 |
| A633D | 90 | 1900 | 1150 |
| A633D | 64 | 2150 | 10200 |
| A633D | 58 | 3900 | 8920 |
| A633D | 40 | 3860 | 1410 |
| A633GrD | 58 | 2600 | 7800 |
| A633GrD | 50 | 2200 | 9000 |
| A633GrD | 45 | 1770 | 6600 |
| A633GrD | 38 | 2500 | 9800 |
| A633GrD | 25 | 2350 | 7650 |
| A633 klas D | 127 | 670 | 1800 |
| A633 klas D | 120 | 3030 | 5400 |
| A633 klas D | 114 | 790 | 4330 |
| A633 klas D | 80 | 3080 | 6090 |
| A633 klas D | 76 | 820 | 2500 |
| A633 klas D | 65 | 2970 | 6720 |
| A633 klas D | 28 | 3360 | 12420 |
| A633 klas D | 24 | 2920 | 9820 |
| Klas E | |
| Kabòn max | 0.22% |
| Manganèz | 1.15-1.50% |
| Fosfò max | 0.030% |
| Souf max | 0.030% |
| Silisyòm | 0.15-0.50% |
| Vanadyòm | 0.04-0.11% |
| Azòt max | 0.03% |

Pwopriyete materyèl
Pwopriyete materyèl sa yo se espesifikasyon ASTM epi yo pral konfime sou Rapò Tès Mill la.
| Klas | Pwen Sede (ksi) | Fòs Tensile (ksi) | Min. 8" % elongasyon |
| A | 42 | 63-83 | 18 |
| C & D Mwens pase oswa egal a 2.5" epè | 50 | 70-90 | 18 |
| C & D >2.5 "epè a 4" epè. | 46 | 65-85 | 18 |
| E Mwens pase oswa egal a 4" epè | 60 | 80-100 | 18 |
| E Plis pase 4" epè a 6" epè. | 55 | 75-95 | 18 |