1. Konpozisyon Chimik ak pwopriyete mekanik
| Egalize | C% | Si% | Mn% | Cr% | Ni% | Mo% | Nb% | V% | P% | S% | Alt% |
| 14cr1mor | 0.05-0.17 | 0.50-0.80 | 0.40-0.65 | 1.15-1.50 | 0.45-0.65 | Mwens pase oswa egal a 0.020 | Mwens pase oswa egal a 0.010 | ||||
| Klas asye | Epesè, nan mm | Fòs rupture | Sede fòs, min | Elongasyon, %, min |
| 14cr1mor | 6<> | 520-680 | 310 | 19 |
| 100<> | 510-670 | 300 |

2.Applications de 14cr1mor asye plak
14cr1mor se souvan itilize nan tank depo petwòl, ekipman echanj chalè, gwo fò tou won reyaksyon, réacteurs, tank depo gwo, plant fòs nikleyè, ekipman chimik, depo ak transpò nan idrid oswa idwojèn medya melanje, ak ekipman ki gen rapò ak sipò, kanalizasyon, ak bouchon nan endistri chimik la.
3. Entwodiksyon nan mwayen - ak segondè - tanperati presyon veso nan GB/T713
GB/T713 clearly defines the grades of medium- and high-temperature pressure vessels, including Q245R, commonly used in boilers, Q345R, used in pressure vessels, as well as 15CrMoR, 12Cr2Mo1R, 12Cr1MoVR, 13MnNiMoR, 18MnMoNbR, Q370R, and Q420R.

4. 14 Cr1mor Espesifikasyon:
Epesè ranje * lajè ranje * longè ranje
8mm-14mm * 2000mm-2500mm * 1800mm-12000mm
16mm-20mm * 2000mm-2500mm * 4500mm-12000mm
22mm-45mm * 1800mm-3000mm * 2550mm-12000mm
50mm-100mm * 1800mm-2800mm * 3500mm-12000mm
105mm-150mm * 2000mm-2500mm * 1800mm-10800mm