JFE-EH360 Plak ki reziste abrasion

JFE-EH360 Plak ki reziste abrasion

Pwodwi: JFE -EH360 plak ki reziste abrasion
Klas: JFE{0}}EH360
Estanda: JIS
Tolerans: ± 1%
Dekri teren
Karakteristik teknik

JFE-EH360 Plak ki reziste abrasion


JFE-EH360 Japonè usure-rezistan asye, JFE-EH360 se plak asye ki reziste -Japon JFE Steel, ak lòt klas JFE-EH400, JFE-EH500, JFE Steel te premye moun ki pwodui plak ki reziste depi nan konmansman an{10}. mwatye nan ane 1950 yo, epi li lajman itilize kòm yon materyèl enpòtan pou machin konstriksyon, machin min, ak machin agrikòl.

 

 
Seri ki disponib nan plak mete JFE-EH360

 

Brinell sifas dite
[garanti]
Non mak Epesè (mm) Kalite Charpy enpak pwopriyete
Charpy absòbe enèji (J)
[garanti]
Tès
tanperati
(degre)
500±40 EVERHARD-C500 5〜101.6 Estanda
Seri
ーーー ーーー
400±30 EVERHARD-C400 5〜101.6
550±40 EVERHARD-C550 5〜32
340±30 EVERHARD-C340 38〜160
450±25 EVERHARD-C450 5〜101.6
Pi gran pase oswa egal a 401 EVERHARD-SP 5〜65 Super Grade ーーー ーーー
450±25 EVERHARD-C450LE 5〜50.8 Seri severite segondè Pi gran pase oswa egal a 27 -40
400±30 EVERHARD-C400LE 5〜60 Pi gran pase oswa egal a 27 -40
500±40 EVERHARD-C500LE 5〜50.8 Pi gran pase oswa egal a 27 -40

 

 
JFE -EH360 abrasion asye plak gwosè

 

  Lajè (mm)
2401
~2600
1801
~2000
1501
~ 1800
2201
~2400
2801
~ 3000
2001
~2200
3001
~ 3200
3201
~3400
3401
~3600
T
h
i
c
k
n
e
s
s
(mm)
22.1~24.0 18 22 24 20 14 22 12 - -
10.0~11.9 14 20 22 16 12 18 - - -
14.0~22.0 14 20 22 16 12 18 - - -
12.0~12.9 14 20 22 16 12 18 - - -
9.0~9.9 12 16 18 12 - 14 - - -
13.0~13.9 14 20 22 16 12 18 - - -
26.1~28.0 22 25 25 24 20 24 18 16 14
30.1~35.0 25 25 25 25 24 25 22 22 22
24.1~26.0 20 24 25 22 16 22 14 12 -
40.1~45.0 25 25 25 25 25 25 25 24 23
28.1~30.0 25 25 25 25 22 25 20 20 18
50.9~60.0 24 23 25 21 20 23 19 18 17
35.1~40.0 25 25 25 25 25 25 24 22 22
70.1~80.0 18 17 19 16 15 17 14 13 13
45.1~50.8 25 25 25 25 25 25 23 22 20
80.1~90.0 16 15 17 14 13 15 13 12 11
60.1~70.0 20 19 22 18 17 20 16 15 14
90.1~100.0 14 13 15 12 12 14 11 10 10

 

 
JFE -EH360 mete plak asye pwodwi aplikasyon

 

JFE-EH360 Japonè Plak asye ki reziste: Li ka itilize pou fabrike ekipman kalite siperyè ak pyès rezèv epi ogmante lavi sèvis yo, diminye risk pou yo pann epi konsa ogmante kapasite pwodiksyon an.JFE-EH360 Plak asye ki reziste pou mete yo ka itilize pou fabrike bokit, chajè, kamyon pil fatra, ékrazan, poudrès ak {5 separator} ki pi popilè. linings.JFE-EH360 Mete Rezistan Steel Plak se kapab kenbe tèt ak nenpòt kalite fwotman ak mete soti nan tout kalite wòch, sab ak fwotman gravye.

 

 
JFE -EH360 mete plak asye pwodwi imaj

 

China abrasion resistant steel sheet Distributors

 

 
Foto ekip gwoup GNEE

 

China abrasion plate Suppliers

 

 
Vizit kliyan gwoup GNEE

 

China abrasion resistant steel sheet Manufacturers

Nou gen ekselan apre-lavant sèvis. Si w gen nenpòt kesyon sou Plak ki reziste JFE-EH360 Abrasion, ou ka kontakte nou epi n ap reponn ou nan dezèdtan.

 

Baj popilè: jfe-eh360 plak ki reziste abrasion, Lachin jfe-eh360 plak ki reziste abrasion manifaktirè, founisè, faktori