Q390b - Q390d cho woule asye wonn ba

Aug 28, 2025 Kite yon mesaj

Q390b - Q390d cho woule asye wonn ba

GB/T1591 Q390 gen senk klas asye diferan kòm Q390A, Q390B, Q390C, Q390D ak Q390E.Structural Steel Q390D dwe fè tès enpak nan tanperati ki ba mwens 20 Degre Centigrade.Normalized tretman chalè sijere yo dwe fè pou asye ki ba plak asye Q390 ki ka fè.

 

info-560-467

Klas asye:

Q390

Aplikasyon:

Asye gwo vitès, asye zouti

Fòm:

Ba wonn

Creole:

Aisi, DIN, JIS, GB

Gwosè:

50mm*50mm-600mm*600mm

Sifas:

Nwa, kale, vire, moulen

Teknik:

Cho woule, fòje

Tès ultrasons:

100% UT pase

 

Dimansyon

 

Cho woule

Fòje

Gwosè (mm)

 

50mm*50mm-600mm*600mm

 

50mm*50mm-600mm*600mm

Longè (mm)

6000 oswa jan sa nesesè

1000-6000

Chimik ak mekanik

Pwopriyete mechnical pou Q390B ba alyaj asye estriktirèl:

Epesè (mm)
Q390B Mwens pase oswa egal a 16 >16 mwens pase oswa egal a 35 >35 mwens pase oswa egal a 50 >50
Sede fòs (pi gran pase oswa egal a MPa) 390 370 350 330
Fòs rupture (MPa) 490-650


Konpozisyon chimik pou Q390B ki ba alyaj asye estriktirèl (analiz chalè max%)

Main eleman chimik konpozisyon nan Q390B
C Si Mn P S V NB Ti Cr NI
0.20 0.55 1.00-1.60 0.040 0.040 0.02-0.20 0.015-0.060 0.02-0.20 0.30 0.70

 

 

info-548-460
Kondisyon teknik ak sèvis adisyonèl:
♦ Tès ba tanperati ki afekte
♦ Koupe ak soude tankou pou chak demand itilizatè fen
♦ Plis striction sou kèk eleman chimik gen ladan
♦ Pibliye Sètifika Egzamen Orginal Mill anba EN 10204 Fòma 3.1/3.2
♦ Tès ultrasons anba GB/T2970, JB4730, EN 10160, ASTM A435, A577, A578